PRECISION IN MATERIAL. CLARITY IN SUPPLY.

GRADE CHART

Stainless steel grade chart and properties

See the properties of austenitic, ferritic, martensitic, duplex and precipitation-hardening (PH) stainless steels in one table. Each rating shows the value behind it. Pick two or three grades to open a detailed comparison.

What is the part for?

61 grades
Stainless steel grade chart: ratings 1–5
HardeningMagnetic
303Austenitic2/5PREN 18.8 · sulphur1/5275 MPa · plate, annealed5/5index 0.854/5type class · sulphur3/5870 °C · continuous, in air—None (cold work)No
304Austenitic3/5PREN 19.31/5270 MPa · plate, annealed3/5index 0.525/5steel type class4/5925 °C · continuous, in airabout the same as 304None (cold work)No
304LAustenitic3/5PREN 19.31/5260 MPa · plate, annealed3/5steel type class5/5steel type class4/5925 °C · continuous, in airabout the same as 304None (cold work)No
321Austenitic3/5PREN 18.01/5250 MPa · plate, annealed3/5steel type class5/5steel type class4/5925 °C · continuous, in air10% dearer than 304None (cold work)No
301Austenitic3/5PREN 19.62/5300 MPa · cold-rolled sheet, annealed3/5steel type class5/5steel type class—5% cheaper than 304None (cold work)No
301LNAustenitic3/5PREN 19.32/5360 MPa · cold-rolled sheet, annealed3/5steel type class5/5steel type class——None (cold work)No
305Austenitic3/5PREN 18.81/5260 MPa · cold-rolled sheet, annealed3/5steel type class5/5steel type class—20% dearer than 304None (cold work)No
347Austenitic3/5PREN 18.01/5260 MPa · plate, annealed3/5steel type class5/5steel type class——None (cold work)No
304CuAustenitic3/5PREN 18.81/5185 MPa · rod, annealed3/5steel type class5/5steel type class——None (cold work)No
316Austenitic, Mo4/5PREN 25.71/5260 MPa · plate, annealed3/5steel type class5/5steel type class4/5925 °C · continuous, in air75% dearer than 304None (cold work)No
316LAustenitic, Mo4/5PREN 26.61/5260 MPa · plate, annealed3/5steel type class5/5steel type class4/5925 °C · continuous, in air75% dearer than 304None (cold work)No
316TiAustenitic, Mo4/5PREN 24.91/5260 MPa · plate, annealed3/5steel type class5/5steel type class—75% dearer than 304None (cold work)No
316L / 316LMoAustenitic, Mo4/5PREN 27.91/5260 MPa · plate, annealed3/5steel type class5/5steel type class4/5925 °C · continuous, in air95% dearer than 304None (cold work)No
Nitronic 50Austenitic, Mo5/5PREN 34.2—3/5steel type class5/5steel type class——None (cold work)No
316LNAustenitic, Mo4/5PREN 29.32/5330 MPa · plate, annealed3/5steel type class5/5steel type class——None (cold work)No
316LVMAustenitic, Mo4/5PREN 27.52/5320 MPa · cold-rolled sheet, annealed3/5steel type class5/5steel type class——None (cold work)No
904LSuper austenitic5/5PREN 36.11/5260 MPa · plate, annealed1/5steel type class3/5steel type class2/5550 °C · sigma phase limit3.1× the price of 304None (cold work)No
254 SMOSuper austenitic5/5PREN 43.32/5320 MPa · plate, annealed1/5steel type class3/5steel type class—3.2× the price of 304None (cold work)No
317LSuper austenitic4/5PREN 30.92/5300 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
317LMNSuper austenitic5/5PREN 35.12/5310 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
310MoLNSuper austenitic5/5PREN 34.51/5280 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
Alloy 926Super austenitic5/5PREN 45.12/5320 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
1.4565Super austenitic5/5PREN 47.12/5440 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
1.4652 (654 SMO)Super austenitic5/5PREN 56.83/5460 MPa · plate, annealed1/5steel type class3/5steel type class——None (cold work)No
310SHeat-resisting austenitic4/5PREN 25.91/5240 MPa · plate, annealed3/5steel type class3/5steel type class5/51050 °C · continuous, in air75% dearer than 304None (cold work)No
309SHeat-resisting austenitic3/5PREN 23.92/5300 MPa · plate, annealed3/5steel type class3/5steel type class4/51000 °C · continuous, in air—None (cold work)No
X15CrNiSi20-12Heat-resisting austenitic3/5PREN 20.91/5270 MPa · plate, annealed3/5steel type class3/5steel type class4/51000 °C · continuous, in air25% dearer than 304None (cold work)No
1.4835 (253 MA)Heat-resisting austenitic3/5PREN 23.62/5370 MPa · plate, annealed3/5steel type class3/5steel type class5/51150 °C · continuous, in air15% dearer than 304None (cold work)No
1.4818 (153 MA)Heat-resisting austenitic3/5PREN 21.62/5340 MPa · plate, annealed3/5steel type class3/5steel type class5/51050 °C · continuous, in air—None (cold work)No
314Heat-resisting austenitic4/5PREN 25.91/5265 MPa · plate, annealed3/5steel type class3/5steel type class5/51150 °C · continuous, in air80% dearer than 304None (cold work)No
430Ferritic2/5PREN 17.02/5365 MPa · cold-rolled sheet, annealed4/5index 0.602/5steel type class3/5815 °C · continuous, in air50% cheaper than 304None (cold work)Yes
1.4104Ferritic1/5PREN 17.8 · sulphur—4/5steel type class1/5type class · sulphur——None (cold work)Yes
441Ferritic3/5PREN 18.02/5310 MPa · cold-rolled sheet, annealed4/5steel type class2/5steel type class—40% cheaper than 304None (cold work)Yes
444Ferritic4/5PREN 24.62/5350 MPa · cold-rolled sheet, annealed4/5steel type class2/5steel type class3/5870 °C · continuous, in air10% dearer than 304None (cold work)Yes
X2CrNi12Ferritic1/5PREN 11.72/5355 MPa · cold-rolled sheet, annealed4/5steel type class2/5steel type class2/5620 °C · continuous, in air55% cheaper than 304None (cold work)Yes
410SFerritic1/5PREN 13.01/5270 MPa · plate, annealed4/5steel type class2/5steel type class——None (cold work)Yes
430NbFerritic2/5PREN 17.02/5320 MPa · cold-rolled sheet, annealed4/5steel type class2/5steel type class——None (cold work)Yes
434Ferritic3/5PREN 20.82/5390 MPa · cold-rolled sheet, annealed4/5steel type class2/5steel type class—25% cheaper than 304None (cold work)Yes
1.4713Ferritic1/5PREN 7.02/5320 MPa · plate, annealed4/5steel type class2/5steel type class3/5800 °C · continuous, in air65% cheaper than 304None (cold work)Yes
1.4742Ferritic3/5PREN 18.02/5375 MPa · plate, annealed4/5steel type class2/5steel type class4/51000 °C · continuous, in air—None (cold work)Yes
1.4762Ferritic4/5PREN 24.52/5405 MPa · plate, annealed4/5steel type class2/5steel type class5/51150 °C · continuous, in air—None (cold work)Yes
410Martensitic1/5PREN 12.52/5300 MPa · plate, annealed3/5index 0.501/5steel type class2/5705 °C · continuous, in air—Quench and temperYes
416Martensitic1/5PREN 14.0 · sulphur2/5350 MPa · rod, annealed5/5index 0.951/5type class · sulphur2/5675 °C · continuous, in air—Quench and temperYes
420 (1.4021)Martensitic1/5PREN 13.03/5500 MPa · rod, annealed2/5steel type class1/5steel type class2/5620 °C · continuous, in air55% cheaper than 304Quench and temperYes
420 (1.4028)Martensitic1/5PREN 13.0—2/5steel type class1/5steel type class2/5620 °C · continuous, in air55% cheaper than 304Quench and temperYes
431Martensitic2/5PREN 16.0—2/5steel type class1/5steel type class3/5870 °C · continuous, in air—Quench and temperYes
440CMartensitic3/5PREN 19.0—2/5steel type class1/5steel type class——Quench and temperYes
415Martensitic—4/5700 MPa · plate, quenched and tempered2/5steel type class1/5steel type class——Quench and temperYes
420 (1.4034)Martensitic1/5PREN 13.52/5375 MPa · cold-rolled sheet, annealed2/5steel type class1/5steel type class2/5620 °C · continuous, in air55% cheaper than 304Quench and temperYes
X50CrMoV15Martensitic2/5PREN 16.92/5390 MPa · cold-rolled sheet, annealed2/5steel type class1/5steel type class——Quench and temperYes
1.4122Martensitic3/5PREN 20.03/5460 MPa · cold-rolled sheet, annealed2/5steel type class1/5steel type class——Quench and temperYes
2304Lean duplex4/5PREN 26.43/5450 MPa · plate, annealed4/5steel type class3/5steel type class1/5250 °C · embrittlement limitabout the same as 304None (cold work)Yes
2101Lean duplex4/5PREN 26.63/5500 MPa · plate, annealed4/5steel type class3/5steel type class1/5250 °C · embrittlement limit25% cheaper than 304None (cold work)Yes
2404Lean duplex5/5PREN 33.03/5520 MPa · plate, annealed4/5steel type class3/5steel type class1/5250 °C · embrittlement limit—None (cold work)Yes
Duplex 2205Duplex5/5PREN 34.53/5510 MPa · plate, annealed3/5index 0.503/5steel type class1/5250 °C · embrittlement limit65% dearer than 304None (cold work)Yes
Super duplex 2507Super duplex5/5PREN 42.13/5580 MPa · plate, annealed1/5steel type class3/5steel type class1/5250 °C · embrittlement limit—None (cold work)Yes
Super duplex S32760Super duplex5/5PREN 41.83/5580 MPa · plate, annealed1/5steel type class3/5steel type class1/5250 °C · embrittlement limit—None (cold work)Yes
17-4 PHPrecipitation hardening (PH)2/5PREN 17.14/5850 MPa · rod, annealed————AgeingYes
15-5 PHPrecipitation hardening (PH)2/5PREN 15.6—————AgeingYes
13-8 Mo PHPrecipitation hardening (PH)3/5PREN 20.3———3/5815 °C · continuous, in air (oxidation only)—AgeingYes
17-7 PHPrecipitation hardening (PH)2/5PREN 17.01/5210 MPa · cold-rolled sheet, annealed————AgeingYes
Sources and technical details

Corrosion: midpoint of the PREN range; thresholds 14 / 18 / 24 / 32. Sulphur-bearing free-machining grades (303, 416, 430F) one step lower. PREN ranks grades and is not a test result in a given environment.

Strength: Outokumpu typical Rp0.2 (MPa) in the stated product and condition; thresholds 300 / 450 / 650 / 900. Standard minimum values are on the grade pages.

Heat resistance: maximum continuous service temperature in dry air (scaling limit; ISER/Euro Inox Table 8, Atlas Figure 11, Outokumpu Table 6:4); for duplex grades the upper limit is 250 °C because of embrittlement (Outokumpu; Atlas 300 °C), for 904L 550 °C because of sigma phase (Atlas). Thresholds 400 / 750 / 900 / 1050 °C. Creep strength must be assessed separately for loaded parts.

Estimated price: five levels from $ (cheap) to $$$$$ (dear); 304 is in the middle ($$$). The level comes from the 12-month average monthly alloy surcharge, which makes up most of the price difference between grades, compared with 304 (under 60 % of 304 is $, under 90 % $$, twice or more $$$$$); the percentage shows on hover and in the comparison tool. Size, quantity, cutting and base price are not included; request a quotation for an exact price.

Machinability: BSSA index (free-machining carbon steel = 1.0) or steel type class. Weldability and magnetism: steel type class (Outokumpu Table 9:1).

Outokumpu — Handbook of Stainless Steel, 2013 (PDF) — Tables 7:5–7:6 typical yield strength; Table 9:1 machinability, weldability and magnetism by steel type; Table 10:1 machinability index (BSSA); p.7: effect of sulphur.

EN 10088-3:2023 and producer datasheets — composition — Composition limits used for PREN; per-grade sources on the grade pages.

Euro Inox / ISER — Stainless Steels at High Temperatures, Table 8 (PDF) — Maximum service temperature in air, intermittent and continuous.

Atlas Steels — Technical Handbook of Stainless Steels, 2021, Figure 11 (PDF) — Maximum service temperature in dry air (ASM Metals Handbook); grade data sheets (2021): 303, 304/304L, 316/316L, 431, 444, 904L, 2205, 2304, 2507, 3CR12.

legierungszuschlag.info — monthly alloy surcharges (December 2025 – November 2026) — Monthly surcharges by grade based on prices published by producers in Germany; 12-month average.

Outokumpu — Monthly Alloy Surcharges for Flat products, December 2024 (PDF) — Cross-check of the ratios.

Carpenter — 440C datasheet (PDF) — Dependence of corrosion resistance on heat treatment.

  • 310S, 309S, X15CrNiSi20-12, 1.4835, 1.4818, 314, 1.4713, 1.4742, 1.4762: Heat-resisting grade, chosen for oxidation resistance at high temperature rather than wet corrosion.
  • 440C: Corrosion resistance depends on heat treatment and drops when annealed or tempered above about 427 °C (Carpenter 440C datasheet). Sources differ in how they compare it with 304.
  • 2304: The machinability rating is the lean duplex type class; the handbook explains it specifically for LDX 2101.
  • 17-4 PH, 15-5 PH, 13-8 Mo PH, 17-7 PH: Corrosion resistance and strength depend on the ageing condition; the table shows the annealed (Condition A) state.
  • Nitronic 50: Nitrogen-strengthened austenitic grade; strength is not in the Outokumpu tables, see the producer data on the grade page.

Frequently asked questions

What are the stainless steel grades and classes?

Stainless steels fall into five families by structure: austenitic (304, 316L), ferritic (430, 444), martensitic (410, 420, 431), duplex (2205, 2507) and precipitation-hardening PH (17-4 PH, 15-5 PH). Each family balances corrosion resistance, strength and machinability differently.

Can stainless steel grades be ranked from best to worst?

There is no single “best” ranking; it depends on the property. In this table corrosion resistance is rated from PREN, strength from typical yield strength, and machinability and weldability from the producer handbook classes, each on a 1–5 scale.

Which stainless steel is the most corrosion resistant?

The five grades with the highest PREN in the table: 1.4652 (56.8), 1.4565 (47.1), Alloy 926 (45.1), 254 SMO (43.3), Super duplex 2507 (42.1). They are super-austenitic and super duplex grades. Results in service also depend on chloride level, temperature and surface condition.

What temperature can stainless steel withstand?

It depends on the grade. In dry air 304 and 316 resist scaling up to about 925 °C in continuous and 870 °C in intermittent service; long exposure at 425–860 °C can lower their wet corrosion resistance. The highest values belong to heat-resisting grades: 1.4835 (1150 °C), 314 (1150 °C), 1.4762 (1150 °C), 310S (1050 °C). Duplex grades are not used above about 250 °C because of embrittlement.

Which stainless steels are magnetic?

Ferritic, martensitic, duplex and PH grades are magnetic. Annealed austenitic grades (304, 316) are not; slight magnetism can appear after cold work.

How can you tell the grade of stainless steel?

The grade is set by composition and cannot be told by eye. A magnet only separates families: annealed 304 is not magnetic and 430 is, though cold-worked 304 can be slightly magnetic. A reliable answer comes from the heat analysis on the EN 10204 3.1 inspection certificate or from a spectrometer (PMI) test.