STAINLESS STEEL FAMILY
Austenitic stainless steels and their properties
Austenitic stainless steels are the most widely used stainless family, valued for forming without cracking and for weldability. 304, 304L, 316 and 316L are its best-known members, used in sheet bodies, pipes and parts machined from bar.
What is austenitic stainless steel?
Austenitic names the internal structure of the metal. These grades contain significant nickel as well as chromium; nickel is one of the main elements that stabilise the austenitic structure. Under EN 10088-3:2023, 1.4301 (304) contains 17.5–19.5 % chromium and 8.0–10.5 % nickel.
Cold bending or drawing can harden these steels and raise their strength; this is called work hardening. Unlike martensitic steels they are not hardened by heating and quenching. They expand more than ferritic families when heated: the typical expansion coefficient at 200–400 °C is about 17–18 × 10⁻⁶/K.
Molybdenum, low carbon and stabilisation
Molybdenum in 316 and 316L adds corrosion resistance in many environments, while sulfur in 303 eases machining. The L in a grade name means low carbon, which limits carbon combining with chromium and lowering corrosion resistance during welding or long heating.
In 321 and 316Ti titanium, and in 347 niobium, binds the carbon; this is stabilisation. Grades such as 904L and 254 SMO are austenitic stainless steels with more nickel and molybdenum than 316L, developed for more demanding environments.
Is austenitic stainless magnetic?
Annealed austenitic grades such as 304 and 316 are generally not attracted to a magnet. After cold working, part of the structure can turn into martensite and the part can be attracted. This does not mean poor quality; a magnet alone cannot identify the grade.
What do the letters LN mean?
L means low carbon and N indicates added nitrogen. All three belong to the austenitic stainless family; austenitic names their steel group. 301LN, 316LN and 317LN share these features, but their chromium, nickel and molybdenum contents differ. They should not be expected to perform identically in the same application. Nitrogen contributes to uses where strength matters alongside corrosion resistance.
What does nitrogen do?
Nitrogen increases the resistance of these stainless steels to permanent deformation under load. In some grades, it also contributes to resistance against corrosion starting at particular points on the surface. Load carrying may be the main concern in a vehicle body, while the effect of the liquid on the metal may matter more in a chemical tank. Nitrogen works together with the other alloying elements.
301LN: rail vehicles and structural parts
301LN / 1.4318 is used in rail vehicles, transport equipment and load-bearing parts. Sheet and strip are product forms used in these applications. Strength matters alongside stainless properties. The weight of a body or support depends on more than metal density: the thickness and cross-section needed to carry the load also affect its weight. This role differs from that of molybdenum-bearing steels for chemical equipment.
316LN: very low-temperature and chemical equipment
316LN is used in equipment operating at very low temperatures, vacuum systems and chemical-processing parts. It belongs to the molybdenum-containing 316 family and combines low carbon with added nitrogen. Molybdenum contributes to corrosion resistance and nitrogen to strength. Its similarity to 316L does not make it the same grade. EN 1.4429 and 1.4406, both associated with 316LN, also have different nickel and molybdenum ranges.
317LN: chemical tanks and tankers
317LN / 1.4434 is used in chemical and petrochemical equipment and tankers carrying chemicals. It contains molybdenum and nitrogen. Unlike 317L, controlled nitrogen addition is part of its grade definition. 317LMN is a separate steel with a different molybdenum range. The concentration and temperature of the liquid matter as well as which liquid contacts the metal.
Shared letters, different jobs
301LN in structures, 316LN at low temperatures and 317LN in chemical equipment serve different needs. The letters LN do not make them interchangeable. These different compositions are one reason stainless steel options extend beyond 304 and 316.
Are 304N and 304LN identical?
304N / 1.4315 and 304LN / 1.4311 are different steels. Both contain nitrogen, but their permitted carbon contents differ. Both may be used where strength matters, without having the same low-carbon requirement. 304N is not another spelling of 304L or 304LN.
| Designation | Maximum carbon | Nitrogen range |
|---|---|---|
| 304N / 1.4315 | 0.06% | 0.12–0.22% |
| 304LN / 1.4311 | 0.03% | 0.12–0.22% |
Sources and technical details
Source: EN 10088-3:2023, Table 2. Values are cast-analysis limits for long products, such as bars, given in mass percent. The nitrogen range is the same in both rows, but the carbon limits differ. This is not one common acceptance requirement for every sheet, bar or ASTM product.
EN 10088-3:2023 — official SIST preview (PDF) — The preview identifies the edition and scope; the numerical rows were checked in Table 2 of the full text. The preview does not contain the entire table.
A tanker wall depends on shape as well as alloy
A chemical tanker wall needs both resistance to the liquid and the ability to carry load. The tanker example considers 316LN / 1.4406 and 317LN / 1.4434 in relation to both needs. Resisting damage from the liquid does not remove the need for the wall to carry its load.
Forming corrugations in flat sheet can increase resistance to bending. In the example bulkheads, the alloy is not the only factor: material, thickness and wall shape work together. This example does not calculate how much thinner sheet could be in a particular tank.
Similar names, different components
304Cu describes copper-bearing stainless steels related to the 304 family. Copper can help form small fasteners and housings without cutting away metal. The trade name does not identify the same composition across every producer. This page follows 1.4567 / X3CrNiCu18-9-4.
303Cu / 1.4570 contains sulfur as well as copper and focuses on machined parts. Both grades are austenitic, a name for their internal structural family. Shared Cu letters do not make the needs of a formed fastener and a turned housing identical.
How does copper affect formability?
These stainless steels can harden as they deform, a behaviour called work hardening. Copper helps reduce this tendency. This is useful when forming a fastener head, hollow housing or complex small part while keeping the metal intact.
305 / 1.4303 also serves forming applications, with a higher nickel content as a distinguishing feature. 305 and 1.4567 can serve similar components while having different compositions. One element alone does not explain their full manufacturing behaviour.
The molybdenum-bearing 1.4578 option
1.4578 combines copper that supports forming with molybdenum. Small connections in chemical and food equipment and formed machine parts are examples. Molybdenum distinguishes its corrosion behaviour from 1.4567. Corrosion is damage caused by metal reacting with substances around it.
Copper and molybdenum do not establish equal resistance at every temperature or in every saline environment. 1.4598 contains both but has a sulfur range aimed at easy cutting and machining. Shared elements do not make the grades interchangeable. The EN number helps distinguish them.
A short comparison of four copper-bearing grades
The table summarises the main application differences. Easy forming, easy cutting and resistance to chemical attack are separate properties. Emphasis on one does not establish equal values for the others. Composition limits and processing conditions appear separately on the grade pages.
| Grade | Distinguishing feature | Application focus |
|---|---|---|
| 1.4567 | Copper-bearing Cr-Ni austenitic | Formed fasteners and small parts |
| 1.4578 | Copper and molybdenum; low sulfur limit | Process components and forming |
| 1.4570 / 303Cu | Sulfur- and copper-bearing | Machining |
| 1.4598 | Contains molybdenum, sulfur and copper | Machined precision components |
Family name and material identity
Trade names such as XM-7, 304Cu and 316Cu can describe a particular producer’s product. Different composition ranges or additional properties may exist within one family name. Properties of one producer’s version therefore do not apply automatically to every similarly named product.
Why does sulphur matter alongside copper?
A small formed connection and a turned housing need different material behaviour. All four grades contain copper, but their sulphur ranges differ. This helps explain the distinction between forming-oriented options and grades that produce readily broken chips.
| Grade | Copper Cu (mass %) | Sulphur S (mass %) |
|---|---|---|
| 1.4567 | 3.00–4.00 | ≤ 0.030 |
| 1.4578 | 3.00–3.50 | ≤ 0.015 |
| 1.4570 / 303Cu | 1.40–1.80 | 0.15–0.35 |
| 1.4598 | 1.30–1.80 | 0.10–0.20 |
Sources and technical details
Source: EN 10088-3:2023, Table 2; cast-analysis limits for long products. “≤” denotes a maximum, not a required actual content. The standard’s footnote attached to the 1.4567 sulphur maximum also describes controlled subranges for different manufacturing purposes. Only Cu and S limits are compared here; full compositions appear on the grade pages.
These percentages alone do not determine cutting speed, forming success or corrosion life. Sulphur’s contribution to chip formation differs from copper’s role in forming; more copper does not automatically mean easier turning.
EN 10088-3:2023 — official SIST preview (PDF) — The preview identifies edition and scope. The numerical comparison follows the Table 2 rows and footnotes in the full text.
Outokumpu — Handbook of Stainless Steel, 2013 (PDF) — PDF pp.14–15: the different roles of copper in forming and sulphur in machining.
Grades in this family
EN, AISI / SAE, UNS and JIS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.
| Grade / Alloy | EN / W.Nr. | AISI / SAE | UNS | JIS | Grade page |
|---|---|---|---|---|---|
| Austenitic stainless steels35 grades | |||||
| Grade page | |||||
| 304General purpose · Forming | 1.4301X5CrNi18-10 | 304 | S30400 | SUS304 | |
| 305Austenitic · High formability | 1.4303X4CrNi18-12 / X5CrNi18-12 | 305 | S30500 | SUS305 | |
| 303Designed for machining | 1.4305X8CrNiS18-9 | 303 | S30300 | SUS303 | |
| 304LLow carbon · General purpose | 1.4307X2CrNi18-9 | 304L | S30403 | SUS304L | |
| 301High strength in cold-worked condition | 1.4310X10CrNi18-8 | 301 | S30100 | SUS301 | |
| 301LNAustenitic · Strength-focused | 1.4318X2CrNiN18-7 | 301LN | S30153 | SUS301L | |
| 316Molybdenum-bearing austenitic | 1.4401X5CrNiMo17-12-2 | 316 | S31600 | SUS316 | |
| 316LMolybdenum alloyed · Low carbon | 1.4404X2CrNiMo17-12-2 | 316L | S31603 | SUS316L | |
| 316LNAustenitic · Low carbon and nitrogen | 1.4429X2CrNiMoN17-13-3 | 316LN | S31653 | SUS316LN | |
| 317LNAustenitic · Molybdenum and nitrogen | 1.4434X2CrNiMoN18-12-4 | 317LN | S31753 | SUS317LN | |
| 316L / 316LMo316L family · Higher Ni and Mo316LMo | 1.4435X2CrNiMo18-14-3 | 316L | S31603 | SUS316L | |
| 317LLow carbon · Increased molybdenum | 1.4438X2CrNiMo18-15-4 | — | S31703 | SUS317L | |
| 317LMNMolybdenum and nitrogen · Low carbon | 1.4439X2CrNiMoN17-13-5 | — | S31726 | — | |
| 316LVMHigh cleanliness · Uniform structure | 1.4441 | — | S31673 | — | |
| 310MoLNAustenitic · Urea and fertiliser applications | 1.4466X1CrNiMoN25-22-2 | — | S31050 | — | |
| S31675High nitrogen · S31675ASTM F1586 · ISO 5832-9 · REX 734 | 1.4472X4CrNiMnMo21-9-4 | — | S31675 | — | |
| Alloy 926Super-austenitic · 6–7% Mo926 | 1.4529X1NiCrMoCuN25-20-7 | — | N08926 | — | |
| 904LHigh-alloy austenitic | 1.4539X1NiCrMoCu25-20-5 | — | N08904 | SUS890L | |
| 321Titanium stabilised | 1.4541X6CrNiTi18-10 | 321 | S32100 | SUS321 | |
| 254 SMOHigh alloy · Chloride resistance | 1.4547X1CrNiMoCuN20-18-7 | — | S31254 | SUS312L | |
| 347Niobium stabilised | 1.4550X6CrNiNb18-10 | 347 | S34700 | SUS347 | |
| 1.4565Super-austenitic · High nitrogen | 1.4565X2CrNiMnMoN25-18-6-5 | — | S34565 | — | |
| 304CuCopper-bearing · Forming applicationsXM-7 | 1.4567X3CrNiCu18-9-4 | — | S30430 | SUSXM7 | |
| 303CuFree machining · Copper bearing303Cu | 1.4570X6CrNiCuS18-9-2 | — | S30331 | — | |
| 316TiMolybdenum + titanium | 1.4571X6CrNiMoTi17-12-2 | 316Ti | S31635 | SUS316Ti | |
| 1.4578Copper and molybdenum · Formability316Cu | 1.4578X3CrNiCuMo17-11-3-2 | — | — | — | |
| 1.4598Molybdenum · Sulfur and copper additions316L+S+Cu | 1.4598X2CrNiMoCuS17-10-2 | — | — | — | |
| 1.4652Super-austenitic · High molybdenum | 1.4652X1CrNiMoCuN24-22-8 | — | S32654 | — | |
| 1.4659Super-austenitic · Tungsten bearing | 1.4659X1CrNiMoCuNW24-22-6 | — | S31266 | — | |
| 1.4818Heat-resistant · UNS S30415 | 1.4818X6CrNiSiNCe19-10 | — | S30415 | — | |
| X15CrNiSi20-12Heat resistant · Silicon bearing | 1.4828X15CrNiSi20-12 | — | — | — | |
| 309SHeat-resistant austenitic stainless | 1.4833X12CrNi23-13 / X7CrNi23-14 | 309S | S30908 | SUH309 | |
| 1.4835Heat-resistant · Nitrogen and silicon bearing | 1.4835X9CrNiSiNCE21-11-2 | — | S30815 | — | |
| 314Heat-resistant grade | 1.4841X15CrNiSi25-21 / X15CrNiSi25-20 | 314 | S31400 | — | |
| 310SHigh-temperature applications | 1.4845X8CrNi25-21 / X12CrNi25-21 | 310S | S31008 | SUS310S | |
Guides
304 vs 316 stainless steel: the differences
304 and 316 are the two most widely used austenitic stainless steels. The main difference is the molybdenum in 316, which improves corrosion resistance in many chloride environments. 304L and 316L are the low-carbon options of the same grades.
Read the guide316L grades: 1.4404, 1.4432 and 1.4435
316L used in tanks, valves and pipes has more than one EN number. Why do the composition differences between 1.4404, 1.4432 and 1.4435 matter in parts contacting chemical liquids?
Read the guide303 and 304L: material differences in machining
303 is useful for easy machining of small fittings and machine parts made in quantity. 304L is prominent in equipment assembled by welding. Sulfur and low carbon explain their value in these different manufacturing duties.
Read the guideStainless steel families and their manufacturing differences
A tank body, pump shaft and cutting component can all be made from stainless steel while needing different properties. Austenitic, ferritic, martensitic, duplex and PH families serve those needs. Their distinctions appear in forming, welding and the development of strength.
Read the guideHow to check stainless steel quality
A magnet does not show the grade. The grade name, the analysis on the EN 10204 3.1 certificate, the lot number on the material and, where needed, XRF or OES analysis are read together.
Read the guideFrequently asked questions
What is austenitic stainless steel?
The stainless family that contains chromium and nickel and can be formed and welded readily. 304, 304L, 316 and 316L are the most common austenitic grades.
What is the difference between 304 and 316?
316 contains molybdenum, which adds corrosion resistance in many environments, particularly chloride-bearing water. 304 has no molybdenum and is common for general use.
What does the L in 304L and 316L mean?
L means low carbon. Low carbon limits carbon combining with chromium and reducing corrosion resistance during welding or long heating.
Does austenitic stainless attract a magnet?
Generally not when annealed. Cold-worked areas can be attracted; this is not a sign of poor quality.
LET’S CLARIFY YOUR REQUIREMENT
Your next project.
The right starting point.
For European-origin material with an EN 10204 3.1 certificate, talk to our team directly about the supply options for your project.
Request a quote