PRECISION IN MATERIAL. CLARITY IN SUPPLY.

STAINLESS STEEL FAMILY

Ferritic stainless steels and their properties

Ferritic stainless steels are a magnetic stainless family that takes its protective surface mainly from chromium. They expand less than austenitic grades when heated and conduct heat better, with uses from appliances to exhaust parts.

What is ferritic stainless steel?

Ferritic names the arrangement of atoms in the metal. The family is chromium-based and, unlike austenitic 304, contains no significant nickel. Compared with common 304 and 316L it expands less and conducts heat better: the typical expansion coefficient at 200–400 °C is about 11 × 10⁻⁶/K.

Ferritic stainless steels are attracted to a magnet. This is a natural property of their structure and does not mean they are not stainless or of low quality.

Where 430, 441 and 444 differ

430 / 1.4016 is a common choice indoors and in relatively mild corrosion conditions, for example appliance panels and kitchen equipment bodies. Molybdenum in 434 / 1.4113 gives better corrosion resistance than 430 in some environments.

441 / 1.4509 is stabilised with titanium and niobium and used in exhaust parts, flue elements and boiler components. 444 / 1.4521 gains resistance to chloride-induced local corrosion from molybdenum; hot-water tanks and heat exchangers are known uses.

Heat-resisting ferritic grades

Ferritic grades such as 1.4742, 1.4762 and 446 / 1.4749 are used in furnace elements, burners and hot-gas parts. Chromium, aluminium and silicon help protect the surface at temperature, and low expansion helps in long, wide parts.

Does a magnet show whether steel is stainless?

Both 441 and 444 are attracted to a magnet. This is a natural feature of their structure, not evidence that they are non-stainless or low-quality materials. Likewise, a metal that is not attracted to a magnet does not automatically offer better corrosion resistance in every environment. Stainless behaviour comes from the alloy composition and its protective surface layer. Magnetism is a separate characteristic. Judging ferritic steels by this simple test alone cannot explain their useful role in heating and water equipment.

Differences from 430 and 316L

430 is a familiar ferritic grade, but it does not have the same stabilising additions as 441 or the molybdenum content of 444. Grade 316L is an austenitic steel containing nickel and molybdenum. Sheets of identical dimensions can consequently look similar while behaving differently under heat or in service. A characteristic that is useful in a hot-gas component may have a different importance in a water tank. These concrete applications make the difference between 441 and 444 easier to understand.

Difference from 430Nb / 1.4511

Grade 430Nb / 1.4511 is a niobium-stabilised ferritic chromium steel associated with exhaust components and thin-section equipment exposed to heat. Although 441 is also stabilised and ferritic, it is a separate EN designation. Molybdenum-bearing 444 addresses a different range of applications with greater corrosion demands.

Grades in this family

15 grades

EN, AISI / SAE, UNS and JIS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.

Material grades: EN, AISI / SAE, UNS and JIS
Grade / AlloyEN / W.Nr.AISI / SAEUNSJISGrade page
Ferritic stainless steels15 grades
Grade page
410SLow carbon · Ferritic1.4000X6Cr13410SS41008SUS410S
405Ferritic · Aluminium bearing1.4002X6CrAl13405S40500SUS405
X2CrNi12Structural ferritic stainless1.4003X2CrNi12 / X2Cr11—S40977—
430Ferritic · General purpose1.4016X6Cr17430S43000SUS430
1.4104Sulfur modified · Machinability1.4104X14CrMoS17———
430FFerritic · Free machining1.4105X6CrMoS17430FS43020—
434Ferritic · Molybdenum bearing1.4113X6CrMo17-1434S43400SUS434
1.4114Ferritic · Molybdenum and sulfur1.4114X6CrMoS19-2———
441Titanium- and niobium-stabilised ferritic4411.4509X2CrTiNb18——SUS430LX
430NbFerritic · Niobium stabilised430LNb · 430 Nb1.4511X3CrNb17——SUS430LX
444Molybdenum-bearing ferritic stainless1.4521X2CrMoTi18-2444S44400SUS444
1.4742Chromium-aluminium-silicon · Ferritic1.4742X10CrAlSi18 / X10CrAl18———
446High-chromium · Heat-resistant ferritic1.4749X18CrN28446S44600SUH446
1.4762High-chromium · Chromium-aluminium-silicon1.4762X10CrAlSi25 / X10CrAl24———
446 / X8Cr24Ferritic · High chromium1.4763X8Cr24446S44600—

Guides

Frequently asked questions

What is ferritic stainless steel?

A chromium-based stainless family without significant nickel that is attracted to a magnet. 430, 441 and 444 are common ferritic grades.

Is ferritic stainless magnetic?

Yes. Ferritic stainless steels are attracted to a magnet because of their structure; this does not mean they are not stainless.

What is the difference between 430 and 304?

430 is ferritic, 304 austenitic. 304 contains significant nickel and covers a wider range of corrosive service; 430 is common indoors and in mild conditions and expands less when heated.

Where is ferritic stainless used?

In appliance and kitchen equipment bodies (430), exhaust and flue parts (441), hot-water tanks (444) and furnace parts (446, 1.4762).

LET’S CLARIFY YOUR REQUIREMENT

Your next project.
The right starting point.

For European-origin material with an EN 10204 3.1 certificate, talk to our team directly about the supply options for your project.

Request a quote