NICKEL ALLOYS
Heat- and corrosion-resistant nickel alloys
The nickel alloys in this family take their strength from composition rather than ageing. Alloy 625 and Hastelloy C-276 are used in chemical equipment; Alloy 600, 601 and Hastelloy X in furnace and hot-gas parts.
Chemical equipment: 625, C-276 and C-22
625 is used in heat exchangers, valves, chemical process piping, marine fittings and bellows. Molybdenum and niobium add strength, and chromium and other additions chemical resistance.
Hastelloy C-22 and C-276 contain nickel, chromium, molybdenum and tungsten. The higher chromium of C-22 helps in oxidising media; molybdenum helps in reducing media and against pitting. Neither is better in every chemical.
Furnaces and hot gas: 600, 601 and X
600 and 601 contain nickel, chromium and iron and are used in furnace linings, hot-gas parts and heat-treatment equipment. Aluminium in 601 helps the protective oxide adhere on surfaces that heat and cool often. Hastelloy X is used in engine parts exposed to hot gas.
Whether the gas is oxidising or reducing, and whether it contains carbon or sulfur, changes how the surface behaves. The same temperature in a different furnace gas can give a different result.
Trade name and grade number
Inconel and Hastelloy are trade names for alloy families, each covering several numbered alloys. Saying “Inconel” alone does not tell whether 600, 625 or 718 is meant. Alloy 625 is EN 2.4856 and UNS N06625.
Corrosion is more than visible rust
Corrosion is damage caused by a metal’s reaction with its environment. It can cause gradual surface loss or small, deep pits. A clean-looking metal does not necessarily resist every environment equally.
Nickel alloys in chemical plants help limit these different effects. Composition changes which liquids and temperatures they can withstand. Corrosion resistance is therefore not one universal number.
What do nickel, chromium and molybdenum contribute?
Nickel forms the main structure of the alloy and contributes to resistance against many chemicals. Chromium helps form a protective surface layer. Molybdenum helps in some acids and against small, deep pits caused by chlorides in salt water. Alloys combine these metals in different proportions.
Pure nickel can be useful in alkaline chemicals, which are chemically opposite to acids. A higher nickel content does not mean better resistance to every chemical. Alloys such as 625 and C-276 are used for the combined contribution of nickel, chromium and molybdenum.
What changes in salt water and tight crevices?
Chlorides in salt water can cause small, deep pits in some metals. Tight regions beneath gaskets receive less fresh liquid and develop conditions different from open surfaces. Crevice corrosion can occur there.
Resistance to these localised forms of corrosion is one reason to use alloys such as 625, C-22 and C-276. A hotter or more concentrated liquid can change their behaviour; exposure matters alongside alloy identity.
Hot-gas oxidation and liquid corrosion
Metal in a chemical liquid works under different conditions from metal exposed to hot furnace gases. Reaction with oxygen forms an oxide layer on the furnace metal: oxidation. Keeping this layer protective matters in furnace alloys. Resistance in acid depends on different chemical conditions.
Resistance of 601 to hot furnace gases and the use of C-276 in chemical equipment are therefore separate properties. Each can be useful in its own environment. Belonging to the nickel family does not establish equal resistance in every environment.
The same liquid can affect a metal differently when heated
In a chemical tank or heat exchanger, a liquid can become hotter without a change in its name or acid concentration. This can change the metal’s surface loss. In the published C-22 example below, every row refers to 10% hydrochloric acid by mass; the test temperature changes.
| Test temperature (°C) | Corrosion rate (mm/year) |
|---|---|
| 38 | 0.01 |
| 52 | 0.28 |
| 66 | 0.98 |
Sources and technical details
Source: Haynes International, C-22, H-2019J, 2023, p.9. The hydrochloric acid is reagent-grade, meaning laboratory purity. The summary does not state specimen product form, processing history, surface preparation or test duration. A process liquid containing other substances may give different results.
mm/year expresses the annual rate of metal loss from the surface. It does not show that the test lasted a year or how long a component will last. It is not the depth of the deepest pit or of damage beneath a gasket. Temperature and the form of damage matter separately, even for the same alloy.
Haynes International — HASTELLOY C-22 (PDF) — P.9: corrosion rates at three temperatures in 10% hydrochloric acid by mass.
Grades in this family
EN, AISI / SAE and UNS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.
| Grade / Alloy | EN / W.Nr. | AISI / SAE | UNS | Grade page |
|---|---|---|---|---|
| Heat- and corrosion-resistant nickel alloys15 grades | ||||
| Grade page | ||||
| Hastelloy C-22Ni-Cr-Mo-W · Mixed process environments | 2.4602 | — | N06022 | |
| Alloy G-30Phosphoric acid applications · High chromium | 2.4603 | — | N06030 | |
| Alloy 686Ni-Cr-Mo-W · Localised corrosion resistance | 2.4606 | — | N06686 | |
| Alloy 333Hot-atmosphere and carburisation resistance | 2.4608 | — | N06333 | |
| Alloy B-2Nickel–molybdenum · Non-oxidising acids | 2.4617 | — | N10665 | |
| Alloy 617High-temperature strength · Oxidation resistance | 2.4663 | — | N06617 | |
| Alloy XHot-gas applications · Oxidation resistance | 2.4665 | — | N06002 | |
| Alloy C-2000Copper-bearing Ni-Cr-Mo · Acid resistance | 2.4675 | — | N06200 | |
| Alloy 230Tungsten bearing · High-temperature strength | 2.4733 | — | N06230 | |
| Alloy 600Solid-solution alloy · Heat and process environments | 2.4816 | — | N06600 | |
| Hastelloy C-276Low C and Si · Demanding chemical processes | 2.4819 | — | N10276 | |
| Alloy 601Aluminium addition · Cyclic oxidation resistance | 2.4851 | — | N06601 | |
| Alloy 625Mo and Nb additions · Corrosion and strength balance | 2.4856 | — | N06625 | |
| Alloy HR-160Sulphur-bearing hot-environment resistance · Nickel–cobalt–chromium | 2.4880 | — | N12160 | |
| Nimonic 75Ni-Cr solid solution · Sheet fabrication and hot service | 2.4951 | — | N06075 | |
Guides
Differences between Alloy 625 and 718
Inconel 625 is prominent in chemical and marine equipment, Inconel 718 in strong engine parts and fasteners. The different purposes behind related names.
Read the guideC-22 and C-276 in chemical tanks and pipework
C-22 and C-276 provide corrosion resistance in chemical tanks, heat exchangers and pipework. Liquid composition, temperature and surface condition after welding affect how the alloys behave.
Read the guideAlloy 600 and 601: furnace applications and differences
Inconel 600 and 601 (Alloy 600 and 601) are used for furnace linings, baskets and supports. Aluminium in 601 helps protect surfaces that frequently heat and cool. Gas composition and the load carried also affect their use.
Read the guideWhat are Inconel, Monel and Hastelloy?
Inconel, Monel and Hastelloy names cover different alloys. 625 can serve chemical equipment, 718 engine parts and Monel 400 marine uses. The number beside the name identifies the particular material.
Read the guideFrequently asked questions
What is Alloy 625?
A nickel-chromium-molybdenum-niobium alloy (2.4856 / N06625) used in heat exchangers, valves, chemical piping and marine fittings.
What is the difference between Hastelloy C-22 and C-276?
Both are nickel-chromium-molybdenum-tungsten alloys. C-22 has more chromium, which helps in oxidising media; which suits better depends on the fluid and temperature.
What is the difference between Alloy 600 and 601?
601 contains aluminium, which helps protective oxide adhere on surfaces that cycle in temperature. 600 combines heat and chemical resistance with good formability and joinability.
LET’S CLARIFY YOUR REQUIREMENT
Your next project.
The right starting point.
For European-origin material with an EN 10204 3.1 certificate, talk to our team directly about the supply options for your project.