NICKEL ALLOYS
Commercially pure nickel: Nickel 200 and 201
Nickel 200 and 201 are commercially pure nickel grades with a high nickel content and small amounts of other elements. They are used in plants producing or handling caustic soda and in parts that conduct heat and electricity.
Properties of pure nickel
Pure nickel resists many alkaline chemicals such as caustic soda. It also conducts heat and electricity well, so it is used in tank surfaces, piping, electrical connections and various parts. Unlike alloys such as 625 and 718, purity, conductivity and alkali resistance matter here more than high strength.
It does not resist every chemical equally. Its behaviour can change with fluid temperature and other constituents; in acid mixtures especially, alloys containing chromium and molybdenum can behave differently.
Nickel 200 versus 201
Nickel 201 contains less carbon. When pure nickel stays hot for long periods, its carbon can separate as graphite and make the metal more brittle; the low carbon of 201 reduces this risk. The difference matters mainly for parts that stay hot; 201 is not a harder or stronger variant.
Use in caustic-soda equipment
Commercially pure nickel can be used for tank parts, heated surfaces, pipework and connections in caustic-soda plants. The liquid’s temperature and other substances within it affect how the material behaves.
Commercially pure nickel is not suitable for every acid or chemical mixture. Alloys containing chromium and molybdenum can be useful in different chemical conditions. A material that performs well in one environment may not do so in another.
Conductivity and product forms
Good electrical conduction is useful in electrical connections, while heated surfaces benefit from heat conduction. Sheet, strip, bar and tube allow these different parts to be made.
If a part stays hot for a long time, the lower carbon in Nickel 201 matters. This difference between Nickel 200 and 201 cannot be seen from appearance or dimensions.
Exposure time and the protective surface film
Under suitable conditions, a protective oxide film can form on commercially pure nickel in contact with caustic soda. This film can slow chemical damage to the metal. The Nickel 201 test below shows why the first day and later days can give different results.
| Test period | Reported annualized corrosion rate (mm/year) |
|---|---|
| First 24 hours | 0.53 |
| After one week, during the following week | 0.07 |
Sources and technical details
Source: Special Metals, Nickel 200 & 201, p.18. Nickel 201 specimens were tested at 420–445°C. The medium is described as 2 kg of technical-grade flake caustic in 500 cm³ of water. An oxide film formed within the first 24 hours. A lower rate was observed after one week, and the test continued for one more week. Specimen dimensions and product form are not stated for this example.
The mm/year unit expresses a short test result as a yearly rate. The specimen was not observed for a year, and a part cannot be expected to lose exactly that thickness each year. This test does not rank Nickel 200 and 201 for corrosion resistance. Different temperatures, impurities or flow conditions can change the result.
Special Metals — Nickel 200 and 201 (PDF) — p.18: oxide-film development in Nickel 201 and the periods of the specified caustic-soda test.
Grades in this family
EN, AISI / SAE and UNS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.
| Grade / Alloy | EN / W.Nr. | AISI / SAE | UNS | Grade page |
|---|---|---|---|---|
| Commercially pure nickel2 grades | ||||
| Grade page | ||||
| Nickel 200Commercially pure nickel · Conductivity and process purity | 2.4060 / 2.4066 | — | N02200 | |
| Nickel 201Low-carbon pure nickel · Selection for hot processes | 2.4061 / 2.4068 | — | N02201 | |
Frequently asked questions
Where is pure nickel used?
In tanks, piping and equipment parts of plants producing or handling caustic soda, and in connections that conduct heat and electricity.
What is the difference between Nickel 200 and 201?
201 contains less carbon, which reduces the risk of graphite separation in parts that stay hot.
Does pure nickel corrode?
It resists corrosion in many alkaline media but not every chemical equally. The result depends on the fluid and temperature.
LET’S CLARIFY YOUR REQUIREMENT
Your next project.
The right starting point.
For European-origin material with an EN 10204 3.1 certificate, talk to our team directly about the supply options for your project.
Request a quote