NICKEL ALLOYS
Nickel superalloys: 718, Waspaloy and Nimonic
Nickel superalloys are nickel-based alloys developed for engine, turbine, ring, shaft and fastener parts that carry load at temperature. The grades on this page gain their strength through an ageing heat treatment.
What is a superalloy?
During ageing very small strengthening particles form inside the metal and make deformation under load harder. In Waspaloy these are gamma prime; in 718 mainly the niobium-bearing gamma double prime (γ″) phase. The particle type and how it changes with temperature are among the reasons the two alloys behave differently after the same treatment.
A short-term force and long-term load at temperature are different cases. Slow deformation of hot metal under load is creep; damage from repeated loading is fatigue. Room-temperature hardness therefore says little about a superalloy.
Welding and heat-treatment sequence
718 is widely used in welded parts. In Waspaloy, residual stress after welding can raise the risk of cracking during later ageing, known as strain-age cracking, so welding and final heat treatment are planned together.
Solution-treated and aged conditions are separate specifications: AMS 5662 and 5663 for 718, AMS 5706 and 5707 for Waspaloy describe different conditions. The stage at which the material is machined affects the result.
Why is melting point not the whole story?
Metal can lose strength long before it melts. Under sustained load it can slowly stretch or bend, known as creep. Repeated loading concerns fatigue. These separate properties matter in heated equipment.
Knowing melting temperature alone does not establish a turbine ring’s load capacity. Superalloys provide options for these hot mechanical duties.
Examples: 718, Waspaloy and Nimonic
718 serves engine rings, casings and high-strength fasteners. Waspaloy, Nimonic 80A and Nimonic 90 also serve loaded engine and turbine parts. Different compositions give different properties and service capabilities.
Hot springs and fasteners are important applications for X-750. A spring needs to retain its force over time as well as be strong. This creates different property needs from a stationary engine casing.
Is every nickel alloy a superalloy?
No. Pure Nickel 200 and 201 serve conductivity and chemical-resistance needs. Invar 36 serves precision dimensions through low expansion. Nickel content alone does not make a material a high-temperature superalloy.
High corrosion resistance alone does not mean high load capacity at temperature. Where a material is used and which properties distinguish it provide more information than the family label alone.
Strength, low weight and stainless properties
Titanium and selected aluminium alloys are known for strength relative to weight. Nickel-base superalloys particularly retain mechanical function at temperature. Different engine regions can therefore use different materials.
PH stainless steels can also gain high strength through ageing heat treatment, which forms small strengthening particles inside the metal. Ageing in both 17-4 PH and 718 does not make their thermal or corrosion properties equal. Corrosion is damage to metal from its surroundings. A similar strengthening route does not establish that different alloys can serve the same duty.
Dimensions can change before a part breaks
Avoiding fracture may not be enough for a hot ring or connection. Stretching under sustained load can also disturb the fit between components. In the producer’s Waspaloy sheet example below, 1% creep and rupture correspond to different stresses at the same 649 °C and 1,000 hours.
| Criterion in the producer table | Approximate initial stress (MPa) |
|---|---|
| Corresponding to 1% creep in 1,000 h | 462 |
| Corresponding to rupture in 1,000 h | 552 |
Sources and technical details
Stress is force per cross-sectional area. MPa is its unit. For the same section, a higher initial stress means a greater tensile force.
Source: Haynes Waspaloy datasheet, 2017, p.4: age-hardened sheet at 649 °C. Specimen treatment: 995 °C/2 h + 845 °C/4 h + 760 °C/16 h, with air cooling after each stage. The table does not state sheet thickness or test direction.
An elongation of 1% means, for example, a 1 mm change over 100 mm; this explanation is not a separate component test. The listed stresses are not short-time tensile strength, design allowable loads or a 1,000-hour life guarantee for every product. They do not transfer directly to other temperatures, durations or product forms.
Haynes — Waspaloy, 2017 (PDF) — p.4: creep and stress-rupture table for sheet specimens; 1% and R rows in the 1,000-hour column.
A hot-gas duct and a turbine ring have different jobs
A sheet that guides hot gas needs to be formed and welded into shape. Parts such as rings, discs or valves may also carry substantial loads while hot. Strength and resistance to repeated loading can be more important in those parts.
Nimonic 75 contains nickel and chromium, resists oxidation in hot environments, and can be formed and welded. In 80A and 90, aluminium and titanium allow strength to be increased through a heat treatment called ageing. This helps explain their different uses.
75: cut, bent and welded sheet bodies
Nimonic 75 sheet is used for protective covers, ducts and bodies of equipment working at high temperatures. Bending can harden the sheet locally. The position of a weld can also affect how the body moves as it heats.
A long sheet expands as it heats. If its connections prevent that movement, additional stresses can build up within it. A thin cover and a thick support therefore have different needs in their shape and connections.
What does ageing do in 80A and 90?
Ageing forms very small particles within the metal. They make it harder for the metal to change shape under load. 80A and 90 develop strength for hot use in this way. Cobalt content is another difference between 90 and 80A.
A short tensile test does not show every aspect of a hot part’s behaviour. Slow deformation under a sustained load is called creep; damage from repeated loads is fatigue. Surface oxidation from hot gases is a separate issue. Different tests examine these properties.
Why is 80A also machined after final heat treatment?
Turning and milling are not always completed while an alloy is soft. Machining 80A in the fully heat-treated condition is also an important production route. Hardness, the load on the cutting tool and cutting conditions matter in this state.
A valve stem, ring and thin-walled body need different holding and finishing arrangements in the machine. Heat treatments specified for bar and sheet can also differ. The processing sequence depends on product form as well as alloy.
What do the composition differences explain?
The table compares titanium, aluminium and cobalt contents in the three alloys. Titanium and aluminium help 80A and 90 develop strength through ageing. The high cobalt content of 90 is another difference from 80A. A larger number in the alloy name does not by itself mean greater strength.
| Grade | Ti, wt. % | Al, wt. % | Co, wt. % |
|---|---|---|---|
| 75 | 0.2–0.6 | Not listed in this table | Not listed in this table |
| 80A | 1.8–2.7 | 1.0–1.8 | ≤ 2.0 |
| 90 | 2.0–3.0 | 1.0–2.0 | 15.0–21.0 |
Sources and technical details
Ti means titanium, Al aluminium and Co cobalt. The figures are selected limits from the p.1 composition table in each Special Metals bulletin. Missing Al or Co limits for 75 do not mean the elements are absent. This short table is not a complete chemical-analysis table for product acceptance. Heat treatment, product form and operating conditions also matter; these figures alone do not establish strength, a welding method or service life.
Special Metals — NIMONIC 75 (PDF) — p.1: titanium range and solid-solution alloy applications; p.3: forming.
Special Metals — NIMONIC 80A (PDF) — p.1: Ti, Al and Co limits; p.21: heat treatment by product form and machining in the fully heat-treated condition.
Special Metals — NIMONIC 90 (PDF) — p.1: Ti, Al and Co limits, age strengthening and hot-load applications.
Grades in this family
EN, AISI / SAE and UNS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.
| Grade / Alloy | EN / W.Nr. | AISI / SAE | UNS | Grade page |
|---|---|---|---|---|
| Nickel superalloys9 grades | ||||
| Grade page | ||||
| Nimonic 90Ni-Cr-Co · Ageing and creep behaviour | 2.4632 / 2.4969 | — | N07090 | |
| Nimonic 263Welded hot structures · Solution treatment and ageing | 2.4650 | — | N07263 | |
| WaspaloyNickel-base superalloy · Hot mechanical strength | 2.4654 | — | N07001 | |
| Alloy 901Age-hardenable · Elevated-temperature strength | 2.4662 | — | N09901 | |
| Alloy 718Precipitation hardening · Condition-dependent properties | 2.4668 | — | N07718 | |
| Alloy X-750Age hardenable · Springs and elevated-temperature loading | 2.4669 | — | N07750 | |
| Alloy 751Age-hardenable · Exhaust-valve applications | 2.4694 | — | N07751 | |
| Nimonic 80ATi-Al age hardening · Elevated-temperature strength | 2.4952 | — | N07080 | |
| Alloy 925Age hardenable · Strength in corrosive service | — | — | N09925 | |
Guides
Alloy 718 and Waspaloy: differences in hot-service use and fabrication
The superalloys Inconel 718 and Waspaloy are used for hot parts such as rings, fasteners and bodies around turbines. They differ in how they behave under load and how they are processed. These differences explain why the same part cannot always be made in the same way from either alloy.
Read the guideDifferences between Alloy 625 and 718
Inconel 625 is prominent in chemical and marine equipment, Inconel 718 in strong engine parts and fasteners. The different purposes behind related names.
Read the guideWhat are Inconel, Monel and Hastelloy?
Inconel, Monel and Hastelloy names cover different alloys. 625 can serve chemical equipment, 718 engine parts and Monel 400 marine uses. The number beside the name identifies the particular material.
Read the guideFrequently asked questions
What are superalloys?
On this page superalloy refers to nickel-based alloys developed for parts that carry load at high temperature and that gain strength by ageing. Alloy 718, Waspaloy, X-750 and Nimonic 80A belong to this group.
Why is Alloy 718 so widely used?
It reaches high strength by ageing and is widely used in welded parts. Turbine and engine parts, rings, shafts and fasteners are its main uses.
What is the difference between 718 and Waspaloy?
Both are age-hardenable nickel alloys but with different strengthening particles. Waspaloy is more prone to cracking when aged after welding; 718 is more common in welded fabrication.
LET’S CLARIFY YOUR REQUIREMENT
Your next project.
The right starting point.
For European-origin material with an EN 10204 3.1 certificate, talk to our team directly about the supply options for your project.
Request a quote