NICKEL ALLOYS
Incoloy and nickel-iron alloys
Nickel-iron alloys contain a high proportion of nickel alongside iron. The Incoloy 800 family is used in chemical equipment, heat exchangers and hot parts; Invar 36, with its low expansion, in fixtures and moulds that must hold dimensions.
Alloy 800, 800H and 800HT
Alloy 800, 800H and 800HT are closely related nickel-iron-chromium alloys with UNS N08800, N08810 and N08811. Base 800 is used in heat-exchanger parts and process piping where heat and chemical resistance matter together.
H and HT are more than names. Carbon content and structure affect load-bearing at temperature; 800HT holds aluminium plus titanium in a narrower range. 800H and 800HT are used in long-term service where creep, slow deformation of hot metal under load, matters.
Invar 36: low expansion
Invar 36 is an iron-nickel alloy that expands very little over certain temperature ranges. It helps hold dimensions in long measuring arms, fixtures and precision moulds. Low expansion does not mean no movement at every temperature.
Where is base Alloy 800 used?
Alloy 800 serves equipment where heat and chemical resistance matter together. Heat-exchanger parts, process tubes and chemical equipment are examples. Its nickel- and chromium-containing structure gives different surface and temperature behaviour from ordinary carbon steels.
A shield in contact with hot gas and a part carrying weight or pressure while hot have different jobs. The loaded part needs to retain shape as well as resist surface exposure. This distinction helps explain the roles of base 800 and the H and HT versions.
Why hot strength matters in 800H and 800HT
Hot metal can gradually bend or stretch under load. This is called creep. 800H and 800HT serve such long-term duties. In a hot furnace or process component, retaining shape matters as well as resistance at the surface.
Carbon content and internal structure affect the ability to carry loads while hot. The combined aluminium and titanium content is also kept within a tighter range in 800HT. These differences do not make one alloy better for every job. They define separate materials for particular long-term temperature and loading conditions.
Oxidation resistance and creep strength are different
Oxidation is a reaction between the metal surface and oxygen. Creep is gradual deformation under heat and load. An alloy’s surface may resist hot gas well, while carrying a load at that temperature needs other properties too.
One general service temperature cannot therefore describe all three alloys. Product form, such as tube or plate, and the job it performs also matter. Each grade page explains its own properties and uses. Similar names do not mean identical properties.
Understanding the three grades side by side
Heat transfer and surface resistance can be central to an exchanger tube. In a furnace part carrying a load while hot for long periods, resistance to gradual deformation also matters. Differences within the 800 family relate to these different duties. The producer’s table below shows the distinctions in carbon and combined aluminium and titanium.
| Grade | UNS | Carbon, wt. % | Al + Ti, wt. % |
|---|---|---|---|
| 800 | N08800 | ≤ 0.10 | 0.30–1.20 |
| 800H | N08810 | 0.05–0.10 | 0.30–1.20 |
| 800HT | N08811 | 0.06–0.10 | 0.85–1.20 |
Sources and technical details
Source: Special Metals, INCOLOY 800H & 800HT bulletin, p.2 Table 1; selected general requirements. The same table gives an average ASTM grain size of 5 or coarser for 800H and 800HT. No grain requirement is stated for base 800. Grains are small crystal regions within the metal.
High-temperature annealing also affects the long-term behaviour of H and HT. Annealing is a heat treatment. Particular applications may have narrower requirements. This summary is not a complete product specification. It does not by itself establish interchangeability or certification to both grades.
Special Metals — INCOLOY 800H & 800HT (PDF) — p.2: composition, grain and application differences; p.3: distinction between short-term mechanical properties and long-term creep behaviour.
Grades in this family
EN, AISI / SAE, UNS and JIS designations of the grades in this family. Designations from different systems do not always imply identical specification requirements.
| Grade / Alloy | EN / W.Nr. | AISI / SAE | UNS | JIS | Grade page |
|---|---|---|---|---|---|
| Incoloy and nickel-iron alloys9 grades | |||||
| Grade page | |||||
| Invar 36Fe-Ni36 · Low thermal expansion | 1.3912 | — | K93600 | — | |
| Alloy DSHot-gas and carburisation resistance | 1.4862 | — | — | — | |
| Alloy 330Heat and carburisation resistance | 1.4864 | — | — | SUH330 | |
| Alloy 800Nickel–iron–chromium · Heat and oxidation resistance | 1.4876 | — | N08800 | NCF800 | |
| Incoloy 800HControlled carbon and grain · Creep-led selection | 1.4958 | — | N08810 | — | |
| Incoloy 800HTN08811 · Controlled chemistry and annealing | 1.4959 | — | N08811 | NCF800H | |
| Alloy 20Sulphuric acid applications · Nickel–iron–chromium | 2.4660 | — | N08020 | — | |
| Alloy HR-120Nickel–iron–chromium · Furnace-atmosphere resistance | 2.4854 | — | N08120 | — | |
| Incoloy 825Titanium stabilised · Wet-corrosion applications | 2.4858 | — | N08825 | — | |
Guides
Invar 36: low expansion and dimensional stability
Invar 36 changes length very little with temperature, making it useful for precision measurement parts and moulds. Machining stresses and connections also affect the dimensions of a finished part.
Read the guideWhat are Inconel, Monel and Hastelloy?
Inconel, Monel and Hastelloy names cover different alloys. 625 can serve chemical equipment, 718 engine parts and Monel 400 marine uses. The number beside the name identifies the particular material.
Read the guideFrequently asked questions
What is the difference between Incoloy 800 and 800H?
800H is defined through carbon content and structure for long-term hot load (creep), UNS N08810. Base 800 (N08800) is used where heat and chemical resistance are needed together.
What is Incoloy?
Incoloy is a trade name for a family of nickel-iron-chromium alloys. 800, 800H, 800HT and 825 are grades known under this name; each number is a separate alloy.
Where is Invar 36 used?
In long measuring arms, fixtures and precision moulds that must keep their dimensions. It expands very little over certain temperature ranges.