GALVANIC CORROSION
Galvanic corrosion chart and galvanic series
Choose two metals in contact to see which one becomes the anode and corrodes, and how far apart they are in the galvanic series. The order follows the seawater galvanic series in MIL-STD-889.
Metals in contact
The order applies to seawater; in air and fresh water the risk is generally lower. For stainless steels “passive” means an intact oxide film, “active” a broken one.
MIL-STD-889
Corrodes: Aluminium 6061-T6
- Anode (active)
- Aluminium 6061-T6
- Cathode (noble)
- Stainless 316L (passive)
- Places apart in the series
- 57 / 91
Galvanic series in seawater
From the most active (anodic) to the most noble (cathodic); the rank is the position in the 92-item MIL-STD-889 series.
Galvanic series (MIL-STD-889, seawater)Metal
| Rank | Metal |
|---|---|
| 1 | Magnesium |
| 4 | Zinc (incl. hot-dip galvanised) |
| 7 | Aluminium 2014-T3 |
| 10 | Cadmium (plated) |
| 13 | Aluminium 5052 |
| 19 | Aluminium 6061-T6 |
| 21 | Aluminium 7075-T6 |
| 25 | Aluminium 2024-T4 |
| 27 | Tin (plated) |
| 28 | Stainless 430 (active) |
| 29 | Lead |
| 30 | Carbon steel (1010) |
| 31 | Cast iron |
| 32 | Stainless 410 (active) |
| 34 | Nickel (plated) |
| 35 | Chromium (plated) |
| 40 | Stainless 304 (active) |
| 49 | Yellow brass |
| 53 | Stainless 316L (active) |
| 54 | Bronze 220 |
| 55 | Copper 110 (Cu-ETP) |
| 59 | Copper-nickel 70/30 (715) |
| 63 | Monel 400 |
| 67 | Stainless 316 (active) |
| 71 | Stainless 304 (passive) |
| 76 | Stainless 316L (passive) |
| 81 | A-286 (passive) |
| 85 | Titanium 6Al-4V |
| 88 | Titanium (CP, 75A) |
| 90 | Silver |
| 91 | Gold |
| 92 | Graphite |
What is galvanic corrosion?
Galvanic corrosion occurs when two dissimilar metals are in electrical contact and share an electrolyte (seawater, moisture, condensation). The more active metal in the series becomes the anode and corrodes faster; the more noble metal becomes the cathode and is protected. If any of the three conditions (dissimilar metals, metal-to-metal contact, a common electrolyte) is missing, galvanic corrosion cannot occur.
How to read the galvanic series
The series runs in seawater from the most active (anodic) to the most noble (cathodic) metal: magnesium and zinc first, aluminium alloys and carbon steel in the middle, passive stainless steels, titanium, silver, gold and graphite at the end. The further apart two metals are, the greater the galvanic corrosion risk usually is. The same stainless steel appears in different places in its passive (intact oxide film) and active states.
How to prevent galvanic corrosion
Choose metals close together in the series; insulate the two metals with plastic washers, sleeves or gaskets; protect the joint from moisture with paint or coating. The anode should be large compared with the cathode: a small aluminium or steel fastener on a large stainless surface corrodes quickly, whereas the reverse is far less risky. Zinc or magnesium sacrificial anodes are used where needed.
Frequently asked questions
Can aluminium be used with stainless steel?
In damp conditions aluminium becomes the anode and corrodes. Indoors and dry the risk is low; outdoors and in marine atmospheres the metals should be insulated and the aluminium area kept larger than the stainless area.
What happens when galvanised steel touches stainless steel?
The zinc coating dissolves as the anode; once it is consumed, the steel beneath corrodes. Use insulating washers when joining galvanised parts with stainless bolts.
Why are copper and aluminium not joined directly?
They are far apart in the series, so aluminium corrodes quickly in damp conditions. Bimetallic (copper–aluminium) transition parts are therefore used in electrical connections.
How is galvanic corrosion prevented?
Choose metals close in the series, insulate them, coat the joint and keep the anode area larger than the cathode. Sacrificial anodes can also be used.