316 better
- 321
- PREN 18.0
- 316
- PREN 25.7
More resistant to pitting; the difference shows in chlorides (salt water, marine air).
GRADE COMPARISON
321 is a titanium-stabilised austenitic stainless steel; 316 contains 2–2.5% molybdenum. Molybdenum gives 316 better pitting resistance in chlorides (PREN 23.1–28.4 against 17–19). The strength of 321 is high temperature: it keeps its resistance to intergranular corrosion after long exposure above 425 °C.
Stainless Steel · 1.4541 · S32100
Stainless Steel · 1.4401 · S31600
Estimated price: reference
No property where it leads
Estimated price: 60% dearer than 321
Equal: Strength · Machinability · Weldability · Heat resistance
316 better
More resistant to pitting; the difference shows in chlorides (salt water, marine air).
316 contains it, 321 does not
Improves resistance to pitting and crevice corrosion in chlorides.
More in 316
Stabilises the austenitic structure; improves toughness and formability.
More in 321
The element that makes steel stainless; more chromium means better corrosion resistance.
| Property | 321 | 316 |
|---|---|---|
| Corrosion | ||
| Strength | ||
| Machinability | ||
| Welding | ||
| Heat | ||
| Estimated price (vs 321) | reference | 60% dearer |
| Critical pitting temperature (ASTM G48 E) | – | 20 °C |
| Critical crevice temperature (ASTM G48 F) | – | <0 °C |
| Tensile strength (Rm) | 570 MPa | 570 MPa |
| Elongation | 55 % | 55 % |
| Hardness | 165 HB | 170 HB |
| Hardening | None (cold work) | None (cold work) |
| Magnetic | No | No |
| Material group | Stainless Steel | Stainless Steel |
| Material no. (W.Nr) | 1.4541 | 1.4401 |
| EN name | X6CrNiTi18-10 | X5CrNiMo17-12-2 |
| AISI | 321 | 316 |
| UNS | S32100 | S31600 |
| JIS | SUS321 | SUS316 |
| Density | 7.9 g/cm³ | 8 g/cm³ |
| PREN | 17–19 | 23.1–28.4 |
Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion
Critical temperatures: Outokumpu Handbook (2013) Table 6:1 typical values; higher is better. They rank grades in a standard test and are not a service limit.
Estimated price: based on the 12-month average alloy surcharge; size, quantity and cutting are not included. How is the price set? · Request a quotation
| Element | 321 | 316 |
|---|---|---|
| C | ≤ 0.08 | ≤ 0.07 |
| Si | ≤ 1 | ≤ 1 |
| Mn | ≤ 2 | ≤ 2 |
| P | ≤ 0.045 | ≤ 0.045 |
| S | ≤ 0.03 | ≤ 0.03 |
| Cr | 17–19 | 16.5–18.5▼ |
| Ni | 9–12 | 10–13▲ |
| Mo | – | 2–2.5▲ |
| N | – | ≤ 0.1 |
| Ti | 5 × C ≤ Ti ≤ 0.70 | – |
Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.
| Property | 321 | 316 |
|---|---|---|
| Modulus of elasticity, GPa | 200 | 200 |
| Thermal expansion 20–200 °C, 10⁻⁶/K | 16.5 | 16.5 |
| Thermal expansion 20–400 °C, 10⁻⁶/K | 17.5 | 17.5 |
| Thermal conductivity, W/(m·K) | 15 | 15 |
| Specific heat, J/(kg·K) | 500 | 500 |
| Electrical resistivity, Ω·mm²/m | 0.73 | 0.75 |
Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator
The compositionally closest grades in the same material group. Choose one to open it as grade 2.
A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.
Choose 316 where the part meets salt water, marine air or chloride chemicals. Choose 321 where it works for long periods at 425–860 °C, as in exhausts, furnaces or hot lines.
Often yes for welded parts near room temperature, as the low carbon of 316L prevents corrosion after welding. For parts working continuously in the sensitisation range, titanium-stabilised 321 is safer.
316 is usually dearer because of its molybdenum; from the last 12 months of alloy surcharges the estimated difference is about 60%. The exact price depends on size and quantity.