More in SAE 4140
- 25CrMo4
- 0.22–0.29
- SAE 4140
- 0.38–0.43
GRADE COMPARISON
4130 and 4140 belong to the same chromium-molybdenum family; the difference is carbon: 0.22–0.29% in 4130 (25CrMo4) and 0.38–0.43% in 4140. More carbon gives 4140 higher hardness and strength after quenching and tempering. 4130 welds more easily, so it is preferred for welded tube structures.
Alloy Steel · 1.7218
Alloy Steel
More in SAE 4140
| Property | 25CrMo4 | SAE 4140 |
|---|---|---|
| Material group | Alloy Steel | Alloy Steel |
| Material no. (W.Nr) | 1.7218 | – |
| EN name | 25CrMo4 | – |
| AISI | 4130 | 4140 |
| UNS | – | – |
| JIS | – | – |
| Density | 7.8 g/cm³ | 7.87 g/cm³ |
| PREN | – | – |
| Element | 25CrMo4 | SAE 4140 |
|---|---|---|
| C | 0.22–0.29 | 0.38–0.43▲ |
| Si | ≤ 0.4 | 0.15–0.35 |
| Mn | 0.6–0.9 | 0.75–1 |
| P | ≤ 0.025 | ≤ 0.035 |
| S | ≤ 0.035 | ≤ 0.04 |
| Cr | 0.9–1.2 | 0.8–1.1 |
| Mo | 0.15–0.3 | 0.15–0.25 |
Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.
The compositionally closest grades in the same material group. Choose one to open it as grade 2.
A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.
4130. Its lower carbon reduces the risk of cracking in the heat-affected zone. Welding 4140 needs preheating and post-weld heat treatment.
Yes. With the same quenching and tempering 4140 reaches higher hardness and tensile strength and hardens through thicker sections.
The closest equivalent of 4130 is 25CrMo4 (1.7218) and of 4140 is 42CrMo4 (1.7225). Composition limits are not identical.