PRECISION IN MATERIAL. CLARITY IN SUPPLY.

GRADE COMPARISON

304 vs 310S stainless steel

310S is a heat-resisting austenitic stainless steel with 24–26% chromium and 19–22% nickel; 304 has 17.5–19.5% and 8–10.5%. The extra chromium and nickel let 310S resist scaling in continuous service in air up to about 1050 °C, against about 925 °C for 304. Room-temperature strength is similar.

Grades to compare

GRADE 1

304

Stainless Steel · 1.4301 · S30400

GRADE 2

310S

Stainless Steel · 1.4845 · S31008

Common comparisons:Duplex 2205 – 316L316Ti – 316L304 – 32117-4 PH – 316410 – 420904L – 316L303 – 4164130 – 4140321 – 316254 SMO – 904L420 – 440C

Key differences

WHERE IT LEADS304

Estimated price: reference

  • Weldability
WHERE IT LEADS310S

Estimated price: 75% dearer than 304

  • Corrosion resistance
  • Heat resistance

Equal: Strength · Machinability

Property differences

Corrosion resistance

310S better

304
PREN 19.3
310S
PREN 25.9

More resistant to pitting; the difference shows in chlorides (salt water, marine air).

Weldability

304 better

304
5/5
310S
3/5

Better suited to welding, with fewer precautions.

Heat resistance

310S better

304
925 °C
310S
1050 °C

Works at higher temperature in air without scaling or embrittlement.

Main composition differences

Nickel (Ni)

More in 310S

304
8–10.5
310S
19–22

Stabilises the austenitic structure; improves toughness and formability.

Chromium (Cr)

More in 310S

304
17.5–19.5
310S
24–26

The element that makes steel stainless; more chromium means better corrosion resistance.

Carbon (C)

More in 310S

304
≤ 0.07
310S
≤ 0.1

Raises strength and hardenability. Low carbon reduces the risk of intergranular corrosion after welding.

Property304310S
Corrosion3/5PREN 19.34/5PREN 25.9
Strength1/5270 MPa · plate, annealed1/5240 MPa · plate, annealed
Machinability3/5index 0.523/5steel type class
Welding5/5steel type class3/5steel type class
Heat4/5925 °C · continuous, in air5/51050 °C · continuous, in air
Estimated price (vs 304)reference75% dearer
Critical pitting temperature (ASTM G48 E)10 °C–
Critical crevice temperature (ASTM G48 F)<0 °C–
Tensile strength (Rm)600 MPa600 MPa
Elongation55 %50 %
Hardness175 HB–
HardeningNone (cold work)None (cold work)
MagneticNoNo
Material groupStainless SteelStainless Steel
Material no. (W.Nr)1.43011.4845
EN nameX5CrNi18-10X8CrNi25-21 / X12CrNi25-21
AISI304310S
UNSS30400S31008
JISSUS304SUS310S
Density7.9 g/cm³7.8 g/cm³
PREN17.5–21.124–27.8

Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion

Critical temperatures: Outokumpu Handbook (2013) Table 6:1 typical values; higher is better. They rank grades in a standard test and are not a service limit.

Estimated price: based on the 12-month average alloy surcharge; size, quantity and cutting are not included. How is the price set? · Request a quotation

Chemical composition, %
Element304310S
C≤ 0.07≤ 0.1▲
Si≤ 1≤ 1.5▲
Mn≤ 2≤ 2
P≤ 0.045≤ 0.045
S≤ 0.03≤ 0.015
Cr17.5–19.524–26▲
Ni8–10.519–22▲
N≤ 0.1≤ 0.11

Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.

Physical properties · 20 °C
Property304310S
Modulus of elasticity, GPa200–
Thermal expansion 20–200 °C, 10⁻⁶/K16.515.5
Thermal expansion 20–400 °C, 10⁻⁶/K17.517.0
Thermal conductivity, W/(m·K)1515
Specific heat, J/(kg·K)500500
Electrical resistivity, Ω·mm²/m0.730.85

Source: EN 10088-1:2005 (Euro Inox tables of technical properties); EN 10095:1999 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator

Alternatives to 304

The compositionally closest grades in the same material group. Choose one to open it as grade 2.

A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.

304 – 310S: C, Si, Cr, Ni

Frequently asked questions

What temperature can 310S withstand?

It resists scaling in continuous service in dry air up to about 1050 °C (Outokumpu). Water vapour and sulphurous gases lower this limit, and creep strength must be checked for loaded parts.

What are the drawbacks of 310S against 304?

Its higher nickel makes it dearer, by an estimated 75%. Long exposure at 650–900 °C can embrittle it through sigma phase. Its chloride resistance at room temperature is not markedly better than 304.

Where is 310S used?

In equipment that runs continuously hot: furnace parts, heat-treatment baskets and fixtures, burner and combustion-chamber parts and heat exchangers.