PRECISION IN MATERIAL. CLARITY IN SUPPLY.

GRADE COMPARISON

303 vs 416 stainless steel

303 and 416 are free-machining stainless steels with added sulphur (S 0.15–0.35%). 303 is austenitic, with better corrosion resistance and no magnetism. 416 is martensitic: it can be hardened, is magnetic and has a slightly higher machinability index (0.95 against 0.85).

Grades to compare

GRADE 1

303

Stainless Steel · 1.4305 · S30300

GRADE 2

416

Stainless Steel · 1.4005 · S41600

Common comparisons:Duplex 2205 – 316L316Ti – 316L304 – 32117-4 PH – 316410 – 420904L – 316L4130 – 4140321 – 316304 – 310S254 SMO – 904L420 – 440C

Key differences

WHERE IT LEADS303
  • Corrosion resistance
  • Weldability
  • Heat resistance
WHERE IT LEADS416
  • Strength

Equal: Machinability

Property differences

Corrosion resistance

303 better

303
PREN 18.8
416
PREN 14.0

More resistant to pitting; the difference shows in chlorides (salt water, marine air).

Strength

416 better

303
275 MPa
416
350 MPa

Higher yield strength; carries the same load with a smaller section.

Weldability

303 better

303
4/5
416
1/5

Better suited to welding, with fewer precautions.

Heat resistance

303 better

303
870 °C
416
675 °C

Works at higher temperature in air without scaling or embrittlement.

Thermal expansion

416 expands less

303
16.5 ×10⁻⁶/K
416
11.0 ×10⁻⁶/K

Changes length less with temperature; matters when joining dissimilar materials and in hot-running parts.

Main composition differences

Nickel (Ni)

303 contains it, 416 does not

303
8–10
416
none

Stabilises the austenitic structure; improves toughness and formability.

Chromium (Cr)

More in 303

303
17–19
416
12–14

The element that makes steel stainless; more chromium means better corrosion resistance.

Carbon (C)

More in 416

303
≤ 0.1
416
0.06–0.15

Raises strength and hardenability. Low carbon reduces the risk of intergranular corrosion after welding.

Property303416
Corrosion2/5PREN 18.8 · sulphur1/5PREN 14.0 · sulphur
Strength1/5275 MPa · plate, annealed2/5350 MPa · rod, annealed
Machinability5/5index 0.855/5index 0.95
Welding4/5type class · sulphur1/5type class · sulphur
Heat3/5870 °C · continuous, in air2/5675 °C · continuous, in air
Tensile strength (Rm)585 MPa550 MPa
Elongation35 %20 %
Hardness––
HardeningNone (cold work)Quench and temper
MagneticNoYes
Material groupStainless SteelStainless Steel
Material no. (W.Nr)1.43051.4005
EN nameX8CrNiS18-9X12CrS13
AISI303416
UNSS30300S41600
JISSUS303SUS416
Density7.9 g/cm³7.7 g/cm³
PREN17–20.612–16

Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion

Chemical composition, %
Element303416
C≤ 0.10.06–0.15▲
Si≤ 1≤ 1
Mn≤ 2≤ 1.5▼
P≤ 0.045≤ 0.04
S0.15–0.350.15–0.35
Cr17–1912–14▼
Ni8–10–▼
Mo–≤ 0.6
N≤ 0.1–
Cu≤ 1–

Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.

Physical properties · 20 °C
Property303416
Modulus of elasticity, GPa200215
Thermal expansion 20–200 °C, 10⁻⁶/K16.511.0
Thermal expansion 20–400 °C, 10⁻⁶/K17.512.0
Thermal conductivity, W/(m·K)1530
Specific heat, J/(kg·K)500460
Electrical resistivity, Ω·mm²/m0.730.60

Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator

Alternatives to 303

The compositionally closest grades in the same material group. Choose one to open it as grade 2.

A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.

303 – 416: C, Mn, Cr, Ni

Frequently asked questions

Is 303 or 416 easier to machine?

416 machines slightly more easily: its BSSA machinability index is 0.95 against 0.85 for 303. Both cut far more easily than standard stainless (304: 0.52).

How to choose between 303 and 416?

Choose 303 for corrosion resistance and a non-magnetic part; 416 for hardness, wear resistance or magnetism. Because of sulphur, neither suits welding or chlorides.

Is 416 magnetic?

Yes, it is martensitic and magnetic. Annealed 303 is not.