PRECISION IN MATERIAL. CLARITY IN SUPPLY.

GRADE COMPARISON

304 vs 321 stainless steel

321 is a titanium-stabilised variant of 304. Because titanium binds carbon, 321 keeps its resistance to intergranular corrosion even after long exposure at about 425–815 °C. At room temperature, corrosion resistance and strength are close.

Grades to compare

GRADE 1

304

Stainless Steel · 1.4301 · S30400

GRADE 2

321

Stainless Steel · 1.4541 · S32100

Common comparisons:Duplex 2205 – 316L316Ti – 316L17-4 PH – 316410 – 420904L – 316L303 – 4164130 – 4140321 – 316304 – 310S254 SMO – 904L420 – 440C

Key differences

WHERE IT LEADS304

Estimated price: reference

No property where it leads

WHERE IT LEADS321

Estimated price: 10% dearer than 304

No property where it leads

Equal: Corrosion resistance · Strength · Machinability · Weldability · Heat resistance

Main composition differences

Nickel (Ni)

More in 321

304
8–10.5
321
9–12

Stabilises the austenitic structure; improves toughness and formability.

Chromium (Cr)

More in 304

304
17.5–19.5
321
17–19

The element that makes steel stainless; more chromium means better corrosion resistance.

Property304321
Corrosion3/5PREN 19.33/5PREN 18.0
Strength1/5270 MPa · plate, annealed1/5250 MPa · plate, annealed
Machinability3/5index 0.523/5steel type class
Welding5/5steel type class5/5steel type class
Heat4/5925 °C · continuous, in air4/5925 °C · continuous, in air
Estimated price (vs 304)reference10% dearer
Critical pitting temperature (ASTM G48 E)10 °C–
Critical crevice temperature (ASTM G48 F)<0 °C–
Tensile strength (Rm)600 MPa570 MPa
Elongation55 %55 %
Hardness175 HB165 HB
HardeningNone (cold work)None (cold work)
MagneticNoNo
Material groupStainless SteelStainless Steel
Material no. (W.Nr)1.43011.4541
EN nameX5CrNi18-10X6CrNiTi18-10
AISI304321
UNSS30400S32100
JISSUS304SUS321
Density7.9 g/cm³7.9 g/cm³
PREN17.5–21.117–19

Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion

Critical temperatures: Outokumpu Handbook (2013) Table 6:1 typical values; higher is better. They rank grades in a standard test and are not a service limit.

Estimated price: based on the 12-month average alloy surcharge; size, quantity and cutting are not included. How is the price set? · Request a quotation

Chemical composition, %
Element304321
C≤ 0.07≤ 0.08
Si≤ 1≤ 1
Mn≤ 2≤ 2
P≤ 0.045≤ 0.045
S≤ 0.03≤ 0.03
Cr17.5–19.517–19▼
Ni8–10.59–12▲
N≤ 0.1–
Ti–5 × C ≤ Ti ≤ 0.70

Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.

Physical properties · 20 °C
Property304321
Modulus of elasticity, GPa200200
Thermal expansion 20–200 °C, 10⁻⁶/K16.516.5
Thermal expansion 20–400 °C, 10⁻⁶/K17.517.5
Thermal conductivity, W/(m·K)1515
Specific heat, J/(kg·K)500500
Electrical resistivity, Ω·mm²/m0.730.73

Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator

Alternatives to 304

The compositionally closest grades in the same material group. Choose one to open it as grade 2.

A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.

304 – 321: Cr, Ni

Frequently asked questions

Why is 321 used for exhausts and hot lines?

When 304 stays at 425–815 °C for long periods, chromium carbides form at grain boundaries and corrosion resistance drops. Titanium in 321 prevents this, so it is preferred for exhaust systems, expansion joints and heat-treatment equipment.

How to choose between 304L and 321?

Both resist intergranular corrosion after welding. 304L is enough near room temperature; 321 is safer for continuous service in the sensitisation range.

Is 321 more corrosion resistant than 304?

Not for general corrosion: PREN values are close (17.5–21.1 for 304, 17–19 for 321). The advantage of 321 is against intergranular corrosion after high-temperature exposure.