904L better
- 904L
- PREN 36.1
- 316L
- PREN 26.6
More resistant to pitting; the difference shows in chlorides (salt water, marine air).
GRADE COMPARISON
904L is a super-austenitic stainless steel with high nickel (24–26%), molybdenum (4–5%) and copper (1.2–2%). This gives it clearly higher resistance than 316L in reducing acids such as sulphuric acid and in chlorides (PREN 32.2–39.9 against 23.1–30). Annealed strength is similar.
Stainless Steel · 1.4539 · N08904
Stainless Steel · 1.4404 · S31603
Estimated price: reference
Estimated price: 45% cheaper than 904L
Equal: Strength
904L better
More resistant to pitting; the difference shows in chlorides (salt water, marine air).
316L better
Easier to machine, with higher cutting speeds and longer tool life.
316L better
Better suited to welding, with fewer precautions.
316L better
Works at higher temperature in air without scaling or embrittlement.
More in 904L
Stabilises the austenitic structure; improves toughness and formability.
More in 904L
Improves resistance to pitting and crevice corrosion in chlorides.
904L contains it, 316L does not
Improves resistance in some acids; gives age hardening in PH grades.
| Property | 904L | 316L |
|---|---|---|
| Corrosion | ||
| Strength | ||
| Machinability | ||
| Welding | ||
| Heat | ||
| Estimated price (vs 904L) | reference | 45% cheaper |
| Critical pitting temperature (ASTM G48 E) | 40 °C | 20 °C |
| Critical crevice temperature (ASTM G48 F) | 10 °C | <0 °C |
| Tensile strength (Rm) | 600 MPa | 570 MPa |
| Elongation | 50 % | 55 % |
| Hardness | 155 HB | 170 HB |
| Hardening | None (cold work) | None (cold work) |
| Magnetic | No | No |
| Material group | Stainless Steel | Stainless Steel |
| Material no. (W.Nr) | 1.4539 | 1.4404 |
| EN name | X1NiCrMoCu25-20-5 | X2CrNiMo17-12-2 |
| AISI | – | 316L |
| UNS | N08904 | S31603 |
| JIS | SUS890L | SUS316L |
| Density | 8 g/cm³ | 8 g/cm³ |
| PREN | 32.2–39.9 | 23.1–30 |
Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion
Critical temperatures: Outokumpu Handbook (2013) Table 6:1 typical values; higher is better. They rank grades in a standard test and are not a service limit.
Estimated price: based on the 12-month average alloy surcharge; size, quantity and cutting are not included. How is the price set? · Request a quotation
| Element | 904L | 316L |
|---|---|---|
| C | ≤ 0.02 | ≤ 0.03 |
| Si | ≤ 0.7 | ≤ 1 |
| Mn | ≤ 2 | ≤ 2 |
| P | ≤ 0.03 | ≤ 0.045 |
| S | ≤ 0.01 | ≤ 0.03 |
| Cr | 19–21 | 16.5–18.5▼ |
| Ni | 24–26 | 10–13▼ |
| Mo | 4–5 | 2–3▼ |
| N | ≤ 0.15 | ≤ 0.1 |
| Cu | 1.2–2 | –▼ |
Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.
| Property | 904L | 316L |
|---|---|---|
| Modulus of elasticity, GPa | 195 | 200 |
| Thermal expansion 20–200 °C, 10⁻⁶/K | 16.1 | 16.5 |
| Thermal expansion 20–400 °C, 10⁻⁶/K | 16.9 | 17.5 |
| Thermal conductivity, W/(m·K) | 12 | 15 |
| Specific heat, J/(kg·K) | 450 | 500 |
| Electrical resistivity, Ω·mm²/m | 1.00 | 0.75 |
Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator
The compositionally closest grades in the same material group. Choose one to open it as grade 2.
A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.
It contains more than twice the nickel and molybdenum, which drive its price. It is also harder to machine.
In sulphuric and phosphoric acid plants, seawater-cooled heat exchangers and environments where 316L suffers pitting.
No. 904L and 316L are austenitic and not magnetic when annealed.