Duplex 2205 is a two-phase stainless steel of austenite and ferrite. With more chromium, molybdenum and nitrogen its PREN is clearly higher than 316L (30.9–38.1 against 23.1–30). Its typical yield strength is about twice as high (510 against 260 MPa), allowing thinner sections.

Grades to compare

GRADE 1

Duplex 2205

Stainless Steel · 1.4462 · S32205

GRADE 2

316L

Stainless Steel · 1.4404 · S31603

Common comparisons:316Ti – 316L304 – 32117-4 PH – 316410 – 420904L – 316L303 – 4164130 – 4140321 – 316304 – 310S254 SMO – 904L420 – 440C

Key differences

WHERE IT LEADSDuplex 2205
  • Corrosion resistance
  • Strength
WHERE IT LEADS316L
  • Weldability
  • Heat resistance

Equal: Machinability

Property differences

Corrosion resistance

Duplex 2205 better

Duplex 2205
PREN 34.5
316L
PREN 26.6

More resistant to pitting; the difference shows in chlorides (salt water, marine air).

Strength

Duplex 2205 better

Duplex 2205
510 MPa
316L
260 MPa

Higher yield strength; carries the same load with a smaller section.

Weldability

316L better

Duplex 2205
3/5
316L
5/5

Better suited to welding, with fewer precautions.

Heat resistance

316L better

Duplex 2205
250 °C
316L
925 °C

Works at higher temperature in air without scaling or embrittlement.

Thermal expansion

Duplex 2205 expands less

Duplex 2205
13.5 ×10⁻⁶/K
316L
16.5 ×10⁻⁶/K

Changes length less with temperature; matters when joining dissimilar materials and in hot-running parts.

Main composition differences

Nickel (Ni)

More in 316L

Duplex 2205
4.5–6.5
316L
10–13

Stabilises the austenitic structure; improves toughness and formability.

Chromium (Cr)

More in Duplex 2205

Duplex 2205
21–23
316L
16.5–18.5

The element that makes steel stainless; more chromium means better corrosion resistance.

Nitrogen (N)

More in Duplex 2205

Duplex 2205
0.1–0.22
316L
≤ 0.1

Raises strength and pitting resistance.

PropertyDuplex 2205316L
Corrosion5/5PREN 34.54/5PREN 26.6
Strength3/5510 MPa · plate, annealed1/5260 MPa · plate, annealed
Machinability3/5index 0.503/5steel type class
Welding3/5steel type class5/5steel type class
Heat1/5250 °C · embrittlement limit4/5925 °C · continuous, in air
Critical pitting temperature (ASTM G48 E)40 °C20 °C
Critical crevice temperature (ASTM G48 F)20 °C<0 °C
Tensile strength (Rm)750 MPa570 MPa
Elongation35 %55 %
Hardness230 HB170 HB
HardeningNone (cold work)None (cold work)
MagneticYesNo
Material groupStainless SteelStainless Steel
Material no. (W.Nr)1.44621.4404
EN nameX2CRNIMON22-5-3X2CrNiMo17-12-2
AISI–316L
UNSS32205S31603
JISSUS329J3LSUS316L
Density7.8 g/cm³8 g/cm³
PREN30.9–38.123.1–30

Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion

Critical temperatures: Outokumpu Handbook (2013) Table 6:1 typical values; higher is better. They rank grades in a standard test and are not a service limit.

Chemical composition, %
ElementDuplex 2205316L
C≤ 0.03≤ 0.03
Si≤ 1≤ 1
Mn≤ 2≤ 2
P≤ 0.035≤ 0.045
S≤ 0.015≤ 0.03
Cr21–2316.5–18.5▼
Ni4.5–6.510–13▲
Mo2.5–3.52–3▼
N0.1–0.22≤ 0.1▼

Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.

Physical properties · 20 °C
PropertyDuplex 2205316L
Modulus of elasticity, GPa200200
Thermal expansion 20–200 °C, 10⁻⁶/K13.516.5
Thermal expansion 20–400 °C, 10⁻⁶/K–17.5
Thermal conductivity, W/(m·K)1515
Specific heat, J/(kg·K)500500
Electrical resistivity, Ω·mm²/m0.800.75

Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator

Alternatives to Duplex 2205

The compositionally closest grades in the same material group. Choose one to open it as grade 2.

A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.

Duplex 2205 – 316L: Cr, Ni, Mo, N

Frequently asked questions

Is duplex better than 316?

In chlorides and where strength matters, yes: it resists pitting and stress corrosion cracking better. 316L is easier to form and weld, and austenitic grades are chosen over duplex for continuous service above about 250 °C.

Is duplex stainless steel magnetic?

Yes. About half of its structure is ferrite, so 2205 is magnetic; annealed 316L is not.

What matters when welding 2205?

Heat input and interpass temperature are limited and a duplex filler is used to keep the ferrite–austenite balance. 316L has no such narrow window.