PRECISION IN MATERIAL. CLARITY IN SUPPLY.

GRADE COMPARISON

420 vs 440C stainless steel

420 and 440C are martensitic stainless steels hardened by heat treatment; they differ in carbon and chromium. 420 (1.4021) has 0.16–0.25% carbon and 12–14% chromium, 440C (1.4125) 0.95–1.2% carbon and 16–18% chromium. The high carbon makes 440C one of the hardest stainless steels, used for bearings, balls and wear parts.

Grades to compare

GRADE 1

420

Stainless Steel · 1.4021 · S42000

GRADE 2

440C

Stainless Steel · 1.4125 · S44004

Common comparisons:Duplex 2205 – 316L316Ti – 316L304 – 32117-4 PH – 316410 – 420904L – 316L303 – 4164130 – 4140321 – 316304 – 310S254 SMO – 904L

Key differences

WHERE IT LEADS420

No property where it leads

WHERE IT LEADS440C
  • Corrosion resistance

Equal: Machinability · Weldability

Property differences

Corrosion resistance

440C better

420
PREN 13.0
440C
PREN 19.0

More resistant to pitting; the difference shows in chlorides (salt water, marine air).

Main composition differences

Carbon (C)

More in 440C

420
0.16–0.25
440C
0.95–1.2

Raises strength and hardenability. Low carbon reduces the risk of intergranular corrosion after welding.

Chromium (Cr)

More in 440C

420
12–14
440C
16–18

The element that makes steel stainless; more chromium means better corrosion resistance.

Molybdenum (Mo)

440C contains it, 420 does not

420
none
440C
0.4–0.8

Improves resistance to pitting and crevice corrosion in chlorides.

Property420440C
Corrosion1/5PREN 13.03/5PREN 19.0
Strength3/5500 MPa · rod, annealed—
Machinability2/5steel type class2/5steel type class
Welding1/5steel type class1/5steel type class
Heat2/5620 °C · continuous, in air—
Tensile strength (Rm)650 MPa–
Elongation20 %–
Hardness––
HardeningQuench and temperQuench and temper
MagneticYesYes
Material groupStainless SteelStainless Steel
Material no. (W.Nr)1.40211.4125
EN nameX20Cr13 / X20Cr14X105CrMo17
AISI420440C
UNSS42000S44004
JISSUS420J1–
Density7.7 g/cm³7.7 g/cm³
PREN12–1417.3–20.6

Ratings are the sourced values of the stainless steel grade chart. Rm, elongation and hardness: Outokumpu typical values at room temperature (HB hot-rolled, HRB cold-rolled product). Grade chart · Hardness conversion

Chemical composition, %
Element420440C
C0.16–0.250.95–1.2▲
Si≤ 1≤ 1
Mn≤ 1.5≤ 1▼
P≤ 0.04≤ 0.04
S≤ 0.03≤ 0.03
Cr12–1416–18▲
Mo–0.4–0.8▲

Arrows mark elements markedly higher (▲) or lower (▼) than in grade 1. Values are the composition limits on the grade pages.

Physical properties · 20 °C
Property420440C
Modulus of elasticity, GPa215215
Thermal expansion 20–200 °C, 10⁻⁶/K11.010.8
Thermal expansion 20–400 °C, 10⁻⁶/K12.011.6
Thermal conductivity, W/(m·K)3015
Specific heat, J/(kg·K)460430
Electrical resistivity, Ω·mm²/m0.600.80

Source: EN 10088-1:2005 (Euro Inox tables of technical properties). Values are for the annealed condition at 20 °C. Thermal expansion calculator

Alternatives to 420

The compositionally closest grades in the same material group. Choose one to open it as grade 2.

A close composition does not make a grade a direct substitute; check mechanical properties, the product standard and the specification.

420 – 440C: C, Mn, Cr, Mo

Frequently asked questions

Is 440C harder than 420?

Yes. With about five times the carbon, hardened 440C reaches clearly higher hardness and wear resistance. 420 is tougher and easier to machine.

Is 440C more corrosion resistant than 420?

It has more chromium, but because of its high carbon the resistance depends on heat treatment and drops when annealed or tempered above about 427 °C (Carpenter 440C datasheet). Hardened 440C tempered at low temperature gives good corrosion resistance compared with 420.

Are 420 and 440C magnetic?

Yes. Both are martensitic and magnetic in every condition.