PRECISION IN MATERIAL. CLARITY IN SUPPLY.

WELDABILITY

Carbon equivalent calculator: CEV, CET and Pcm

Enter the steel’s chemical composition to see its carbon equivalent (CEV, CET, Pcm) and a weldability rating. For alloy steels you can also search for a grade to see the CEV range from its composition limits.

Chemical composition (%)

Enter the weight per cent values from the heat analysis; leave absent elements at 0. Carbon equivalents are for carbon and low-alloy steels.

CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15

Carbon equivalent

0.41CEV (IIW) · weldability: Good
CET (EN 1011-2)
0.32
Pcm (Ito–Bessyo)
0.26
CEV 0.41 · CET 0.32 · Pcm 0.26

Carbon equivalent of alloy steels

CEV, CET and Pcm of the alloy steels on this site, calculated from the composition limits on each grade page.

Carbon equivalent by gradeCEV · CET · Pcm
GradeCEVCETPcm
H111.770.790.81
1.47131.20–1.890.30–0.620.32–0.60
300M VAR0.920.620.62
4330M0.75–0.960.47–0.600.42–0.53
4340 Air Melt0.860.590.53
4340 VAR0.860.590.53
HP9-4-301.270.670.57
Nitriding 135M0.890.580.54
SAE 41400.70–0.870.51–0.610.47–0.56
SAE 93100.660.300.26

What is the carbon equivalent?

The carbon equivalent converts the effect of the alloying elements on hardenability into a single carbon content. The higher it is, the greater the risk of a hard, brittle heat-affected zone after welding and of hydrogen cracking. It is therefore used to judge weldability and the need for preheat.

Carbon equivalent formulas

The most common is the IIW formula: CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. It is method A of EN 1011-2 and is given as the maximum CEV of EN 10025 structural steels. CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40 is used for preheat in method B of EN 1011-2. Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B (Ito–Bessyo) is preferred for modern low-carbon steels with about 0.11% C or less.

How to read weldability

A common reading of CEV: up to 0.35 excellent, 0.36–0.40 very good, 0.41–0.45 good, 0.46–0.50 fair and above 0.50 poor weldability. The higher the value, the more preheat, low-hydrogen consumables and controlled heat input are needed. The actual preheat depends not only on composition but on thickness, heat input and hydrogen level, and should be set to EN 1011-2. Carbon equivalents are not used for stainless steels.

Frequently asked questions

How is the carbon equivalent calculated?

With the IIW formula: CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15, elements in weight per cent. For C 0.18, Mn 1.40 and the others 0, CEV = 0.18 + 0.233 = 0.41.

At what carbon equivalent is preheat needed?

As a general guide, preheat and low-hydrogen welding are needed once CEV rises above about 0.45; thick sections may need it at lower values. The preheat temperature is set to EN 1011-2 together with thickness, heat input and hydrogen level.

What is the difference between CEV and Pcm?

CEV was developed for carbon, carbon-manganese and low-alloy steels. Pcm better reflects hydrogen cracking risk in modern low-carbon (about 0.11% or less) microalloyed steels, for which CEV can overstate the risk.