HARDNESS CONVERSION

HRB to HB conversion chart

Convert HRB to an approximate HB value, or the other way round. Choose the material group; HRB – HB tables for steel and stainless follow below.

MEASURED HARDNESS

Scale and value

Hardness scale

Table range: 61–100 HRB. A decimal comma or point is accepted.

Approximate comparison for stainless steels. Not a grade-specific measurement.

Table scope

Uses a general stainless steel comparison dataset. Grade and material condition can affect the relationship within this group. It does not apply to another metal family.

HARDNESS COMPARISONS

Approximate conversion

HRCRockwell C

—

No table comparison
HRBRockwell B

90

Your input
HBBrinell

≈192

Approximate comparison
HVVickers

≈203

Approximate comparison

Estimated tensile strength

UTS · N/mm² (MPa)

≈ 652 N/mm²

A material-dependent estimate; not a replacement for a tensile test or certificate result.

HRC: — HRB: 90 HB: ≈ 192 HV: ≈ 203 Estimated tensile strength (UTS): ≈ 652 N/mm²

Hardness conversion tableHRC · HRB · HB · HV · Estimated UTS

The selected row, or two adjacent rows used in calculation, are highlighted. A dash indicates an unavailable comparison.

Approximate comparison for stainless steels. Not a grade-specific measurement.
HRCRockwell CHRBRockwell BHBBrinellHVVickersUTSEstimated · N/mm²
57——640—
56——615—
54.5——591—
53.5——569—
52——547—
51——528—
49.5——508—
48.5——4911539
47—4444741520
45.5—4294551471
44.5—4154401422
43—4014251363
42—3884101314
40.5—3753961265
39—3633831236
38—3523721187
36.5—3413601157
35.5—3313501118
34.5—3213391089
33—3113281049
32—3023191020
31—293309990
30—285301971
29—277292941
27.5—269284912
26.5—262276892
25.5100255269873
2499248261853
2398241253824
2297235247794
20.596229241775
——223235755
—95217228745
—94212223716
—93207218696
—91197208667
—89187197637
—87179189608
—85170179559
—83163172539
—81156165530
—79149157500
—77143150481
—74137144471
—72131138461
—69126133451
—67121127431
—64116122422
—61111117402
——107113382
——103108373
Sources and technical details

Numerical table source: BSSA — stainless steel hardness comparison. The source defines the scope of the approximate comparison; it is not a test result for a particular component.

HRB to HB conversion chart

Rows are the measured comparison points the calculator uses, read in both directions: find HRB in the first column for HB, or HB in the second column for HRB. Values between rows are interpolated by the calculator above.

HRB – HB: carbon and low-alloy steelapproximate; reference points of the calculator
HRBHB
99.5238
98.1228
96.7219
96214
95209
94204
93.5199
92.5195
91.5190
89.5181
87.1171
85162
81.7152
78.7143
75133
71.2124
66.7114
62.3105
56.295
5290
4886
4181
HRB – HB: stainless steelapproximate; reference points of the calculator
HRBHB
100255
99248
98241
97235
96229
95217
94212
93207
91197
89187
87179
85170
83163
81156
79149
77143
74137
72131
69126
67121
64116
61111

Worked examples

  1. 70 HRB → ≈ 128 HB in stainless.
  2. 85 HRB → ≈ 162 HB in carbon steel, ≈ 170 HB in stainless.
  3. 95 HRB → ≈ 209 HB in carbon steel, ≈ 217 HB in stainless.

What are HRB and HB?

HRB (Rockwell B) is read from the indentation depth of a 1/16 in (1.588 mm) ball under a 100 kgf total load; it is used for softer materials such as mild steel, brass and aluminium.

HB (Brinell) is calculated from the diameter of the impression of a hard metal ball (for steels usually 10 mm and 3000 kgf); its large impression gives an average value on castings and coarse structures. With a hard metal ball the result is also written HBW.

How do you convert HRB to HB?

There is no exact formula between HRB and HB; the two tests use different indenters and loads. Conversion uses comparison tables measured on both scales for the same material group. A value on a table row is read directly; one between two rows is interpolated between those rows only.

The result is approximate and depends on the material group. For acceptance or certificates, measure the required scale directly.

Valid range of the chart

The carbon and low-alloy steel chart covers 41–99.5 HRB and 81–238 HB; the stainless steel chart covers 61–100 HRB and 111–255 HB. No conversion is given outside these ranges.

Frequently asked questions

What is 90 HRB in HB?

About 192 HB for stainless steel. The value is approximate and depends on the material group.

What is 192 HB in HRB?

About 91.9 HRB for carbon and low-alloy steel and about 90 HRB for stainless steel. The reverse conversion reads the same comparison table.

Is there a formula from HRB to HB?

There is no universal formula. Conversion relies on comparison tables measured on both scales for the same material group, and the tables differ by material.

Is the HRB to HB conversion the same for stainless?

Not exactly; each material group has its own chart. For 90 HRB: about 192 HB for stainless steel. Choose the material group in the calculator.

What is the difference between HRB and HB?

HRB (Rockwell B) is read from the indentation depth of a 1/16 in (1.588 mm) ball under a 100 kgf total load; it is used for softer materials such as mild steel, brass and aluminium. HB (Brinell) is calculated from the diameter of the impression of a hard metal ball (for steels usually 10 mm and 3000 kgf); its large impression gives an average value on castings and coarse structures. With a hard metal ball the result is also written HBW.